MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

ChevronTexaco 220 Honor Ashless AW
Categories: Fluid; Lubricant

Material Notes:

Texaco Honor Ashless AW are circulating oils formulated from high quality base stocks and a carefully balanced, zinc-free additive package. These proved excellent protection against wear for long bearing and gear life. Texaco Honor Ashless AW have superior water separability properties and rust protection to deal with the severe water contamination that frequently occurs in circulating oil systems. Their outstanding oxidation stability minimize deposit formation and lead to long lubricant life.

Texaco Honor Ashless AW are circulating oils designed for the steel mill industry. They are formulated to meet the needs of circulation systems serving high-speed rollers and plain bearings in no-twist finishing mills. They are also recommended for the lubrication of reduction gears and bearings where zinc-free oils are desired. They meet the requirements of Morgan Construction Company Morgoil Lubricant Spec REv. 1.0a and Danieli Corporation 0.000.002 standard.

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

CPS Number: 227293; MSDS Number: 8912

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
API Gravity 27.8 °27.8 °
Viscosity Measurement 9696Viscosity Index
Saybolt Viscosity at 100°F 1103 SUS1103 SUS
Saybolt Viscosity at 210°F 93.3 SUS93.3 SUS
Kinematic Viscosity at 40°C (104°F) 209 cSt209 cSt
Kinematic Viscosity at 100°C (212°F) 18.2 cSt18.2 cSt
 
Thermal PropertiesMetricEnglishComments
Pour Point -5.00 °C23.0 °F
Flash Point 278 °C532 °F
 
Descriptive Properties
Rust PreventionPass

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Techmer ES HiFill FR® PC GF20 FR 20% Glass Filled
ChevronTexaco 320 Honor Ashless AW
Aluminum 6063-T6
Aluminum 5052-H32
304 Stainless Steel (UNS S30400); 1/8 Hard Bar, Plate, Sheet, and Strip

WTEXA092 / 76971

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.