MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

High-leaded brass, UNS C34200, OSO25 Temper flat products
Categories: Metal; Nonferrous Metal; Copper Alloy; Brass

Material Notes: Fair to excellent corrosion resistance. Combines excellent machinability with moderate cold workability.

Applications: gears, wheels, nuts, plates for clocks, keys, bearing cages, engraver's plates.

Test specimen: flat product - 1mm thickness.

Key Words: CZ119, ISO CuZn35Pb2, CEN CW601N, free-cutting brass
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.50 g/cc0.307 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell F 7676
Hardness, Rockwell 30T 3737
Tensile Strength, Ultimate 360 MPa52200 psi
Tensile Strength, Yield 140 MPa
@Strain 0.5 %
20300 psi
@Strain 0.5 %
Elongation at Break 48 %48 %In 50 mm
Modulus of Elasticity 105 GPa15200 ksi
Poissons Ratio 0.3460.346
Machinability 90 %90 %UNS C36000 (free-cutting brass) = 100%
Shear Modulus 39.0 GPa5660 ksi
Shear Strength 250 MPa36300 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000660 ohm-cm
@Temperature 20.0 °C
0.00000660 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 20.3 µm/m-°C
@Temperature 20.0 - 300 °C
11.3 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.380 J/g-°C0.0908 BTU/lb-°F
Thermal Conductivity 115 W/m-K
@Temperature 20.0 °C
798 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point 885 - 910 °C1630 - 1670 °F
Solidus 885 °C1630 °F
Liquidus 910 °C1670 °F
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 425 - 600 °C797 - 1110 °F
Hot-Working Temperature 785 - 815 °C1450 - 1500 °F
Recrystallization Temperature 320 °C608 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 62.5 - 66.5 %62.5 - 66.5 %
Iron, Fe <= 0.10 %<= 0.10 %
Lead, Pb 1.5 - 2.5 %1.5 - 2.5 %
Other, total <= 0.50 %<= 0.50 %
Zinc, Zn 33.5 %33.5 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
High-leaded brass, UNS C34200, OSO35 Temper flat products
High-leaded brass, UNS C34200, OSO15 Temper flat products
Low-silicon bronze B, UNS C65100, H00 Temper 2 mm wire
Medium-leaded brass, UNS C34000, H00 Temper wire
Nickel Aluminum Bronze, UNS C63000, HR50 Temper

MC34200b3 / 11202

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.