MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Geon® Performance Solutions Vinyl Packaging VEO-184 Polyvinyl Chloride, Rigid
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Rigid Grade

Material Notes:

Geon Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.33 g/cc1.33 g/ccASTM D792
Apparent Bulk Density 0.801 g/cc0.0289 lb/in³ASTM D1505
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8383ASTM D2240
Tensile Strength, Yield 52.4 MPa7600 psiType I, 5.1 mm/min; ASTM D638
Flexural Strength 75.8 MPa11000 psiASTM D790
Flexural Modulus 1.41 GPa205 ksiASTM D790
Izod Impact, Notched 10.0 J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
18.7 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 82 %
@Thickness 0.851 mm,
Wavelength 700 nm
82 %
@Thickness 0.0335 in,
Wavelength 700 nm
Internal Method
 
Processing PropertiesMetricEnglishComments
Processing Temperature 193 - 210 °C379 - 410 °FBlow Molding
 
Descriptive Properties
AppearanceClear/Transparent
FeaturesGeneral Purpose
 High Gloss
 Medium Impact Resistance
FormsPellets
Generic MaterialPVC, Rigid
Generic NamePolyvinyl Chloride, Rigid (PVC, Rigid)
Processing MethodProfile Extrusion
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesGeneral Purpose
 Packaging

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Geon® Performance Solutions Vinyl Rigid Molding M3900 Polyvinyl Chloride, Rigid
Colorite Polymers 2002 Rigid PVC
Axiall 9109J Clear Rigid PVC, Extrusion, Clear
Colorite Polymers 2007 Rigid PVC
Geon® Performance Solutions Vinyl Fittings M1012 Polyvinyl Chloride, Rigid

PH0POL0346 / 144915

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.