MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow H349-02 Polypropylene Homopolymer Resin  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Extrusion Grade; Polypropylene, Film Grade

Material Notes: H349-02 Polypropylene Resin intended for use in biaxial oriented (BOPP) film processes. This product can also be used in extrusion and thermoforming applications where improved melt strength is desired.

Main Characteristics

  • Good gauge control
  • High drawability
  • Good optics
  • Complies with U.S. FDA 21 CFR 177.1520(c)1.1a

Braskem acquired Dow's polypropylene business. This specific grade was discontinued priot to the acquisition and so is listed as a discontinued Dow product.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D792
Melt Index of Compound 2.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 32.4 MPa4700 psiASTM D638
Elongation at Yield 12 %12 %ASTM D638
Flexural Modulus, 1% Secant 1360 MPa197000 psiASTM D790
Izod Impact, Notched  0.214 J/cm
@Temperature 0.000 °C
0.401 ft-lb/in
@Temperature 32.0 °F
ASTM D256A
 0.480 J/cm
@Temperature 23.0 °C
0.899 ft-lb/in
@Temperature 73.4 °F
ASTM D256A
 
Thermal PropertiesMetricEnglishComments
Melting Point 160 °C320 °FDSC; Dow Method
Deflection Temperature at 0.46 MPa (66 psi) 87.2 °C189 °FUnannealed; ASTM D648
 
Optical PropertiesMetricEnglishComments
Haze 46 %
@Thickness 1.00 mm
46 %
@Thickness 0.0394 in
ASTM D1003
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Braskem H 504 XP Bioriented Film Polypropylene
Carmel Olefins Capilene® E 65 F Polypropylene Homopolymer
Carmel Olefins Capilene® G 86 E Polypropylene Homopolymer
Dow H110-02N Polypropylene Homopolymer Resin
Phillips 66 COPYLENE® CH016 Polypropylene, Homopolymer, BOPP

PDOW0975 / 93311

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.