MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Spartech SP-3810 TPO/TPE Polyolefin Sheet
Categories: Polymer; Thermoplastic; Polyethylene (PE); TPO

Material Notes: Description: Polyolefin Sheet

Information provided by Spartech.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.11 g/cc1.11 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6969ASTM D2240
Tensile Strength at Break 15.9 MPa2300 psiASTM D638
Elongation at Break 375 %375 %ASTM D638
Flexural Modulus 1.38 GPa200 ksiASTM D790
Dart Drop 12.6 g/micron320 g/mil73°F; ASTM D3029
 
Thermal PropertiesMetricEnglishComments
CTE, linear 55.8 µm/m-°C
@Temperature 20.0 °C
31.0 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 52.8 °C127 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polypropylene, Sheet/Thermoforming Grade
Borealis Daplen™ AK4504 TPO Compound
Spartech Royalite R59 ABS/PVC Fire Rated Sheet
Borealis Daplen™ ED213AE TPO Compound
Spartech Formalloy HG High-Gloss TPO Alloy Specialty Sheet

PSPAR081 / 68522

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.