MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Syensqo (Solvay Specialty Polymers) Kalix® 3950 Polyamide, High Performance (HPPA), 50% Glass Fiber  (discontinued **)
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 50% Glass Fiber Reinforced

Material Notes: Kalix® 3950 is a 16% bio-sourced, amorphous polyphthalamide (PPA)-based compound with 50% by weight glass fiber reinforcement. This material is uniquely formulated to prevent warpage and flash in parts produced using the injection molding process. Its high stiffness, strength, and impact resistance in comparison to other highly reinforced grades of polyamide characterize the material. The material has been specifically developed to provide a high quality surface finish and fill thin-wall section parts such as those used in mobile electronic devices. The material also provides excellent stain resistance in comparison to other polyamide-based materials.

Features: Good Dimensional Stability; Good Impact Resistance; Good Surface Finish; High Flow; High Stiffness; High Strength; Hot Water Moldability; Low Warpage; Minimal Flash; Paintable; Platable; Stain Resistant

Uses: Cell Phones; Electrical Parts; Electrical/Electronic Applications; Thin-walled Parts

Injection Molding Notes: Kalix® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Kalix® resins be dried prior to molding.

Additional Properties: Biobased Content - ASTM D6866 16 %

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.58 g/cc0.0571 lb/in³ASTM D792
Filler Content 50 %50 %Glass Fiber
Water Absorption 0.16 %
@Time 86400 sec
0.16 %
@Time 24.0 hour
ISO 62
Linear Mold Shrinkage, Flow 0.00010 cm/cm0.00010 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0014 cm/cm0.0014 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 239 MPa34700 psiISO 527-2
Elongation at Break 2.2 %2.2 %ISO 527-2
Tensile Modulus 16.7 GPa2420 ksiISO 527-2
Flexural Strength 346 MPa50200 psiISO 178
Flexural Modulus 16.1 GPa2340 ksiISO 178
Izod Impact, Notched (ISO) 15.0 kJ/m²7.14 ft-lb/in²Type 1, Notch A; ISO 180
Izod Impact, Unnotched (ISO) 70.0 kJ/m²33.3 ft-lb/in²ISO 180
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 4.18
@Frequency 2.40e+9 Hz
4.18
@Frequency 2.40e+9 Hz
ASTM D2520
Dissipation Factor 0.012
@Frequency 2.40e+9 Hz
0.012
@Frequency 2.40e+9 Hz
Method B; ASTM D2520
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 145 °C293 °FHDT B; Unannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 137 °C279 °FUnannealed; ISO 75-2/A
Glass Transition Temp, Tg 144 °C291 °FDSC
Flammability, UL94 HB
@Thickness >=0.600 mm
HB
@Thickness >=0.0236 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 270 °C518 °F
Front Barrel Temperature 300 °C572 °F
Melt Temperature 310 - 330 °C590 - 626 °F
Mold Temperature 80.0 - 130 °C176 - 266 °F
Drying Temperature 80.0 °C
@Time 14400 - 43200 sec
176 °F
@Time 4.00 - 12.0 hour
Moisture Content <= 0.090 %<= 0.090 %
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 North America
ColorBlack; Natural; White
FormPellets
Part Marking Code>PA10I/10T/X-GF50<ISO 11469
Processing TechniqueInjection Molding; Water-Heated Mold Injection Molding

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company RTP 2099 X 126216 D Bio-Based Polylactic Acid (PLA); Fast-Cycle Nucleator - Glass Fiber - 59% Renewable Resource Content
EMS-Grivory Grilamid® XE 4116 nat PA1010-GF55
RTP Company RTP 2099 X 121249 D Bio-Based Polylactic Acid (PLA); Standard Nucleator - Glass Fiber - 58% Renewable Resource Content
Syensqo (Solvay Specialty Polymers) Kalix® 3850 Polyamide, High Performance (HPPA), 50% Glass Fiber
RTP Company RTP 2099 X 124790 C Bio-Based Polylactic Acid (PLA); Impact Modified - Mineral - Standard Nucleator - 78% Renewable Resource Content

PSOL8Y7159 / 176890

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.