MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Teknor Apex Telcar® TL-2683C Thermoplastic Elastomer
Categories: Polymer; Thermoplastic

Material Notes: Telcar TL-2683C is a general purpose thermoplastic polyolefin elastomer designed for automotive applications and is suitable for injection molding and extrusion.

Availability: Asia Pacific

Uses: Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Sporting Goods; Weatherstripping

RoHS Compliant:RoHS

Form: Pellets

Processing Method: Injection Molding; Extrusion

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.892 g/cc0.0322 lb/in³ASTM D792
Melt Flow 20 g/10 min
@Load 2.16 kg,
Temperature 230 °C
20 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5656ASTM D2240
Tensile Strength at Break 16.5 MPa2390 psiASTM D412
Elongation at Break 500 %500 %ASTM D412
 
Processing PropertiesMetricEnglishComments
Processing Temperature 188 - 210 °C370 - 410 °FInjection, Melt
Rear Barrel Temperature 171 - 193 °C340 - 380 °FInjection
Middle Barrel Temperature 177 - 199 °C350 - 390 °FInjection
Front Barrel Temperature 182 - 204 °C360 - 400 °FInjection
Nozzle Temperature 188 - 210 °C370 - 410 °FInjection
Zone 1 166 - 188 °C330 - 370 °FExtrusion
Zone 2 171 - 193 °C340 - 380 °FExtrusion
Zone 3 177 - 199 °C350 - 390 °FExtrusion
Zone 5 182 - 204 °C360 - 400 °FExtrusion
Die Temperature 190 - 210 °C374 - 410 °FExtrusion
Mold Temperature 25.0 - 65.6 °C77.0 - 150 °FInjection
Injection Pressure 1.38 - 6.89 MPa200 - 1000 psiInjection
Back Pressure 0.172 - 0.345 MPa25.0 - 50.0 psiInjection
Cushion 0.381 - 2.54 cm0.150 - 1.00 inInjection
Screw Speed 30 - 100 rpm30 - 100 rpmExtrusion
 50 - 100 rpm50 - 100 rpmInjection
 
Descriptive Properties
AppearanceOpaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Teknor Apex Telcar® TL-2468A Thermoplastic Elastomer
Teknor Apex Telcar® TL-2478K Thermoplastic Elastomer
Teknor Apex Telcar® TL-1000-105 Thermoplastic Elastomer

PTEKNQ1660 / 238151

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.