MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

INEOS Styrolution Terluran® EHI-4 NR ABS Extrusion Application
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes:

Information provided by STYROLUTION, which is a joint venture between BASF and INEOS

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.02 g/cc0.0368 lb/in³ASTM D792
Melt Flow 3.06 g/10 min
@Load 10.0 kg,
Temperature 220 °C
3.06 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 39.0 MPa5660 psi2in/min; ASTM D638
Tensile Modulus 1.78 GPa258 ksiASTM D638
Flexural Modulus 1.78 GPa258 ksiASTM D790
Charpy Impact, Notched  9.60 J/cm²
@Temperature -40.0 °C
45.7 ft-lb/in²
@Temperature -40.0 °F
ASTM D256
 33.5 J/cm²
@Temperature 23.0 °C
159 ft-lb/in²
@Temperature 73.4 °F
ASTM D256
Dart Drop, Total Energy 31.0 J22.9 ft-lbASTM D3763
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 93.0 °C
@Load 5.10 kg
199 °F
@Load 11.2 lb
Rate 50°C/hr; ASTM D1225
 
Descriptive Properties
Commercial StatusNorth America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Elix Polymers ELIX ABS E401 Acrylonitrile Butadiene Styrene (ABS), Extrusion, Impact Grade
LG Chemical LI960 ASA, Extrusion
INEOS Styrolution Terluran® EGP-7 ABS
INEOS Styrolution Terluran® GP-22 ABS
INEOS Styrolution Terluran® GP-25 ABS

PBASG0611 / 132244

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.