MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ipiranga Petrochem GM 5240 PR HDPE  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Pipe Grade

Material Notes: IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.

To produce HDPE, IPQ employs Hoechst/Hostalen technology through the following steps: the ethene supplied by COPESUL is processed by Ipiranga Petroquímica in reactors to produce powdered polyethylene. The polyethylene then receives additives and is homogenized with stabilizers and taken to extruding presses where it is granulated and is ready for marketing.

An integrated and computerized system controls the production, from the initial processing stages to end-product testing for later commercialization.

Applications:

  • conduits for optic fiber
  • geomembranes
  • jacketing of optics cables and metallic (telecommunication)
  • pipes for optic fiber
  • three layer coating of metallic pipes (gas pipelines)
  • umbilicals for offshore oil field platforms

Ipiranga Petrochem polymer product lines have been acquired by Braskem.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.953 - 0.961 g/cc0.0344 - 0.0347 lb/in³ASTM D792-98
Melt Flow 0.39 - 0.71 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.39 - 0.71 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238-00
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 23.0 MPa3340 psiASTM D638-02
Elongation at Yield 8.9 %8.9 %ASTM D638-02
Flexural Modulus 0.840 GPa
@Strain 2 %
122 ksi
@Strain 2 %
Secant; ASTM D790-02
Izod Impact, Notched 0.900 J/cm1.69 ft-lb/inASTM D256-03

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Renegade Materials Corporation RM-3002 Bismaleimide (BMI) Resin 4581 Astroquartz III
ExxonMobil Escorene® HD-8761 HDPE, Rotational Molding Powder
ExxonMobil Escorene® HD-8661 HDPE, Rotational Molding Powder
Ethydco Advancene™ EE-4010-AAH HDPE Pipe Extrusion
Ethydco Advancene™ bEE-4906-AAH HDPE Pipe Extrusion

PIPIRA26 / 48359

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.