MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil Exxsol™ D110 Dearomatized Fluid
Categories: Fluid

Material Notes: Availability: Asia Pacific, Central America, North America and South America

Appearance: Clear/Transparent Liquid

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.808 g/cc
@Temperature 15.6 °C
0.0292 lb/in³
@Temperature 60.0 °F
ASTM D4052
Kinematic Viscosity 3.43 cSt3.43 cStASTM D445
Vapor Pressure <= 0.000133 bar
@Temperature 20.0 °C
<= 0.100 torr
@Temperature 68.0 °F
ExxonMobil Method
 
Thermal PropertiesMetricEnglishComments
Boiling Point 248 °C478 °FInitial; ASTM D86
Flash Point 114 °C237 °FMethod A; ASTM D93
 
Descriptive Properties
Aniline Point181°FMethod E, ASTM D611
Aromatic Content (%)0.4ExxonMobil Method
Dry Point509°FASTM D86

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Exxsol™ D100 Dearomatized Fluid
ChevronTexaco Superla® 5 White Oil
ExxonMobil Exxsol™ D120 Dearomatized Fluid

PEX99587 / 175823

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.