MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Nanocyl PLASTICYL™ PA1501 Polyamide 66 with 2 wt% Multi-Wall Carbon Nanotubes
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: PLASTICYL™ is a family of Multi-Wall Carbon Nanotube (MWNT) thermoplastic concentrates for applications requiring superior electrical conductivity and electrostatic discharge (ESD) properties. PLASTICYL™ PA1501 is a conductive masterbatch based on polyamide 66. Because of its flow formulation, PLASTICYL™ PA1501 is ideal for standard injection molding and extrusion processes.

Applications:

  • ESD (Electrostatic Discharge) and electrically conductive parts
  • E&E, automotive, industrials
  • Injection molding, extrusion

Benefits:

  • Electrical conductivity at low loading
  • Retention of key mechanical properties
  • Easier processing

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Filler Content 2 %2 %Carbon Nanotube Loading
Melt Flow 29.18 g/10 min
@Load 1.20 kg,
Temperature 300 °C
29.18 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ISO 1133:1997
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 71.88 MPa10430 psiISO 527-1,2
Elongation at Break 2.56 %2.56 %ISO 527-1,2
Tensile Modulus 3.205 GPa464.9 ksiISO 527-1,2
Charpy Impact, Notched 0.500 J/cm²2.38 ft-lb/in²ISO 180
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 6.78e+8 ohm-cm6.78e+8 ohm-cmCTM E043
 
Thermal PropertiesMetricEnglishComments
Melting Point 263 °C505 °FMasterbatch; ISO 11357-1,-3
 
Processing PropertiesMetricEnglishComments
Processing Temperature 300 °C572 °FMaterial Temperature
Hold Pressure 25.0 MPa3630 psi
Back Pressure 0.000 MPa0.000 psi
 
Descriptive Properties
Processing: Holding Time25 s
Processing: Injection Speed70 cm³/s
Processing: Plasticizing Speed0.4 m/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Envalior Akulon® Ultraflow™ K-FG6 Nylon 6-30% Glass Reinforced (European Grade) (Dry)
Envalior Akulon® S223-D Nylon 66 (European Grade) (Dry)
Envalior Akulon® S223-D Nylon 66 (European Grade) (Cond)
Avient Lubri-Tech™ NT-05KV15GF/000 Nylon 6/6, Glass Filled
Nanocyl PLASTICYL™ PA1501 Polyamide 66 with 3 wt% Multi-Wall Carbon Nanotubes

PNANOCY979 / 108934

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.