MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company EMI 2861-60A Thermoplastic Polyolefin Elastomer (TEO); Stainless Steel Fiber - Electrically Conductive - EMI/RFI Shielding
Categories: Polymer; Thermoplastic; Elastomer, TPE; Olefinic TPE

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.02 g/cc1.02 g/ccASTM D 792
Additive Loading 10 %10 %Primary Additive
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 606010 s delay; ASTM D 2240
Tensile Strength at Break 1.62 MPa235 psiASTM D 412
Elongation at Break 140 %140 %ASTM D 412
Tear Strength 13.1 kN/m75.0 pliDie C; ASTM D 624
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 100 ohm-cm<= 100 ohm-cmASTM D 257
Surface Resistance <= 1000 ohm<= 1000 ohmESD STM11.11
Surface Resistivity per Square <= 10000 ohm<= 10000 ohmASTM D 257; ESD STM11.11
Static Decay <= 0.50 sec<= 0.50 secFTMS101C; 4046.1
Shielding Effectiveness  45 dB
@Thickness 3.00 mm,
Frequency 5.00e+8 Hz
45 dB
@Thickness 0.118 in,
Frequency 5.00e+8 Hz
ASTM D 4935
 47 dB
@Thickness 3.00 mm,
Frequency 7.00e+8 Hz
47 dB
@Thickness 0.118 in,
Frequency 7.00e+8 Hz
ASTM D 4935
 48 dB
@Thickness 3.00 mm,
Frequency 3.00e+8 Hz
48 dB
@Thickness 0.118 in,
Frequency 3.00e+8 Hz
ASTM D 4935
 50 dB
@Thickness 3.00 mm,
Frequency 1e+9 Hz
50 dB
@Thickness 0.118 in,
Frequency 1e+9 Hz
ASTM D 4935
 51 dB
@Thickness 3.00 mm,
Frequency 1.30e+9 Hz
51 dB
@Thickness 0.118 in,
Frequency 1.30e+9 Hz
ASTM D 4935
 53 dB
@Thickness 3.00 mm,
Frequency 1.50e+9 Hz
53 dB
@Thickness 0.118 in,
Frequency 1.50e+9 Hz
ASTM D 4935
 
Processing PropertiesMetricEnglishComments
Melt Temperature 182 - 210 °C360 - 410 °F
Mold Temperature 15.6 - 65.6 °C60.0 - 150 °F
Drying Temperature 79.4 °C
@Time 7200 sec
175 °F
@Time 2.00 hour
Moisture Content 0.030 %0.030 %
Dew Point -17.8 °C0.000 °F
Injection Pressure 82.7 - 124 MPa12000 - 18000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Premix Thermoplastics PRESEAL® TPE 5020
Avient Stat-Tech™ UR-7SS-5GF/000 PT GY Thermoplastic Elastomer - TPU, Glass Filled
RTP Company ESD C 2800 B-75A Black Thermoplastic Polyolefin Elastomer (TEO), Electrically Conductive - ESD Protection
RTP Company Permaprene™ 2800 B-85A Thermoplastic Polyolefin Elastomer (TEO)
Multibase Multi-Flex® D 3104-8 TPO Thermoplastic Polyolefin Elastomer

PQZRA35759 / 206144

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.