MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

SunChemical Gwent C2090819P2 Silver Ink
Categories: Fluid; Metal; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: This product is part of a range of Heat Curable Inks designed specifically for use in Photovoltaic panels. These products are based on a unique curing process that results in the low temperature formation of a thermosetting polymer. This ink has excellent adhesion, chemical and environmental resistance properties.
Excellent adhesion to glass
Screen Printing Equipment: semi-automatic, manual
Screen Types: stainless steel, polyester, mesh 156 to 325tpi
Substrate: Glass

Information provided by Gwent Electronic Materials Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 57 - 59 %
@Temperature 700 °C
57 - 59 %
@Temperature 1290 °F
Viscosity 8000 - 10500 cP
@Shear Rate 230 1/s,
Temperature 25.0 °C
8000 - 10500 cP
@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT 550 PK1.1°
Thickness 23.0 microns0.906 milCured film on glass
Storage Temperature 20.0 °C68.0 °Fsealed container
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 0.15 ohm
@Thickness 0.0250 mm
0.15 ohm
@Thickness 0.000984 in
Normalized, Cured on glass
 
Processing PropertiesMetricEnglishComments
Cure Time  3.00 min
@Temperature 130 °C
0.0500 hour
@Temperature 266 °F
belt dryer
 30.0 min
@Temperature 130 °C
0.500 hour
@Temperature 266 °F
box oven
Shelf Life 6.00 Month6.00 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
SunChemical Gwent C2030701D3 Solderable Silver Ink
SunChemical Gwent C2100203D2 Silver Ink
SunChemical Gwent C2090210P12 Silver Ink
SunChemical Gwent C2050712D58 Silver Ink for ITO Substrates
SunChemical Gwent C2040712D5 Ink Jet Printable Silver Ink

WGELZ9033 / 139346

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.