MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polymer Resources NY6-IM1 Nylon 6, Impact Modified
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Impact Grade

Material Notes: Nylon 6, Impact Modified

Process: Injection Molding
Notes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).

Information provided by Polymer Resources Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.09 g/cc1.09 g/ccASTM D792
Linear Mold Shrinkage 0.016 - 0.020 cm/cm0.016 - 0.020 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 62.1 MPa9000 psiASTM D638
Tensile Strength, Yield 62.1 MPa9000 psiASTM D638
Flexural Strength 75.8 MPa11000 psiASTM D790
Flexural Modulus 2.07 GPa300 ksiASTM D790
Izod Impact, Notched 1.60 J/cm
@Temperature 22.8 °C
3.00 ft-lb/in
@Temperature 73.0 °F
ASTM D256
Gardner Impact 36.2 J26.7 ft-lbASTM D3029
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 168 °C335 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 62.8 °C145 °FASTM D648
Flammability, UL94  HB
@Thickness 1.59 mm
HB
@Thickness 0.0626 in
 HB
@Thickness 3.17 mm
HB
@Thickness 0.125 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 221 - 246 °C430 - 475 °F
Middle Barrel Temperature 238 - 254 °C460 - 490 °F
Front Barrel Temperature 243 - 260 °C470 - 500 °F
Melt Temperature 238 - 268 °C460 - 515 °F
Mold Temperature 65.6 - 82.2 °C150 - 180 °F
Drying Temperature 73.9 - 85.0 °C165 - 185 °F
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hour
Vent Depth 0.000762 cm0.000300 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Polymer Resources PC-HH Polycarbonate, High Heat

PPOLYQ074 / 160590

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.