MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Arkema KYNAR® 761 Polyvinylidene Fluoride Powder
Categories: Polymer; Thermoplastic; Fluoropolymer; Polyvinylidene Fluoride (PVDF); Polyvinylidinefluoride (PVDF), Molded/Extruded

Material Notes: Characteristics: White, non-hygroscopic powder. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistance; high purity

Applications:

  • Chemical processing – production, storage and transfer of corrosive fluids
  • Electronics – protective sheathing, plenum and wiring insulation
  • Semi-conductor industry
  • Food stuff and Healthcare industries
  • Transportation – fuel line and pipe, thermoformed body components

Information provided by Arkema Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.77 - 1.79 g/cc1.77 - 1.79 g/ccASTM D792
Density 1.78 g/cc0.0643 lb/in³Melt
Water Absorption 0.010 - 0.030 %0.010 - 0.030 %ASTM D570
 0.020 %0.020 %Dry; Sim. to ISO 62
Viscosity 2.30e+6 - 2.90e+6 cP
@Shear Rate 100 1/s,
Temperature 230 °C
2.30e+6 - 2.90e+6 cP
@Shear Rate 100 1/s,
Temperature 446 °F
Melt; ASTM D3835
Linear Mold Shrinkage, Flow 0.030 cm/cm0.030 in/inDry; ISO 294-4, 2577
 0.030 cm/cm0.030 in/in
Melt Flow  1.3 g/10 min
@Load 10.0 kg,
Temperature 230 °C
1.3 g/10 min
@Load 22.0 lb,
Temperature 446 °F
cm³/10 min Volumetric Rate; ISO 1133
 2.0 - 6.0 g/10 min
@Load 12.5 kg,
Temperature 230 °C
2.0 - 6.0 g/10 min
@Load 27.6 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 76 - 8076 - 80ASTM D2240
Tensile Strength at Break 34.5 - 55.2 MPa5000 - 8010 psiASTM D638
Tensile Strength, Yield 44.8 - 55.2 MPa6500 - 8010 psiASTM D638
 50.0 MPa7250 psiDry; ISO 527-1/-2
Elongation at Break >= 50 %>= 50 %Dry; ISO 527-1/-2
 20 - 100 %20 - 100 %ASTM D638
Elongation at Yield 5.0 - 10 %5.0 - 10 %ASTM D638
 9.0 %9.0 %Dry; ISO 527-1/-2
Tensile Modulus 1.38 - 2.31 GPa200 - 335 ksiASTM D638
 2.00 GPa290 ksiDry; ISO 527-1/-2
Flexural Strength 58.6 - 75.8 MPa
@Strain 5.0 %
8500 - 11000 psi
@Strain 5.0 %
ASTM D790
Flexural Modulus 1.38 - 2.31 GPa200 - 335 ksiASTM D790
Compressive Strength 68.9 - 103 MPa9990 - 14900 psiASTM D695
Izod Impact, Notched 0.961 - 2.14 J/cm1.80 - 4.01 ft-lb/inASTM D256
Izod Impact, Unnotched 10.7 - 42.7 J/cm20.0 - 80.0 ft-lb/inASTM D256
Charpy Impact, Notched 5.00 J/cm²
@Temperature 23.0 °C
23.8 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179/1eA
Coefficient of Friction, Dynamic 0.140.14vs. steel; ASTM D1894
Coefficient of Friction, Static 0.200.20vs. steel; ASTM D1894
Taber Abrasion, mg/1000 Cycles 5.0 - 9.05.0 - 9.0CS 17 1000g:pad; ASTM-G195-13A
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.00e+14 ohm-cm2.00e+14 ohm-cm65% R.H; ASTM D257
Dielectric Constant 4.5 - 9.5
@Frequency 1000 Hz
4.5 - 9.5
@Frequency 1000 Hz
ASTM D150
Dissipation Factor 0.010 - 0.21
@Frequency 100000 Hz
0.010 - 0.21
@Frequency 100000 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 119 - 144 µm/m-°C66.1 - 80.0 µin/in-°FASTM D696
CTE, linear, Parallel to Flow 150 µm/m-°C83.3 µin/in-°FDry; ISO 11359-1/-2
Specific Heat Capacity 0.745 - 0.958 J/g-°C0.178 - 0.229 BTU/lb-°FDSC
Thermal Conductivity 0.170 - 0.190 W/m-K1.18 - 1.32 BTU-in/hr-ft²-°FASTM D433
 0.190 W/m-K1.32 BTU-in/hr-ft²-°FMelt
Melting Point 165 - 172 °C329 - 342 °FASTM D3418
 170 °C338 °F10°C/min; Dry; ISO 11357-1/-3
Maximum Service Temperature, Air 150 °C302 °FUL RTI
Deflection Temperature at 0.46 MPa (66 psi) 125 - 140 °C257 - 284 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 104 °C219 °FDry; ISO 75-1/-2
 105 - 115 °C221 - 239 °FASTM D648
Glass Transition Temp, Tg -40.0 °C-40.0 °F10°C/min; Dry; ISO 11357-1/-2
 -40.6 - -38.3 °C-41.1 - -36.9 °FASTM D7028
Decomposition Temperature 375 °C707 °F1% wt. loss, TGA, in air
 410 °C770 °F1% wt. loss, TGA, in nitrogen
UL RTI, Electrical 150 °C302 °FUL 746B
UL RTI, Mechanical without Impact 150 °C302 °FUL 746B
Flammability, UL94 V-0V-0Yellow Card Available; Dry; IEC 60695-11-10
 V-0
@Thickness 0.800 mm
V-0
@Thickness 0.0315 in
IEC 60695-11-10
Oxygen Index 43 %43 %Dry; ISO 4589-1/-2
 44 %44 %ASTM D2863
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.421.42sodium D line; ASTM D542
 
Processing PropertiesMetricEnglishComments
Melt Temperature 190 - 270 °C374 - 518 °F
Mold Temperature 20.0 - 90.0 °C68.0 - 194 °F
 
Descriptive Properties
Form as DeliveredPowder
Moisture SensitiveNo
Processing MethodsOther Extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arkema Kynar® HSV 1800 PVDF
Arkema KYNAR® 760 Polyvinylidene Fluoride Homopolymer - Extrusion
Arkema KYNAR® 370 Polyvinylidene Fluoride (PVDF) Homopolymer - Injection Molding
Arkema Kynar® 710 Polyvinylidene Fluoride Homopolymer- Injection Molding
Arkema KYNAR FLEX® 3120-50 Polyvinylidene Fluoride Copolymer - Extrusion & Molding

PARKG934 / 144559

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.