System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Envalior Pocan® B 1100 000000 PBT
Categories:
Polymer
;
Thermoplastic
;
Polyester, TP
;
Polybutylene Terephthalate (PBT)
;
Polybutylene Terephthalate (PBT), Unreinforced, Molded
Material Notes:
PBT, non-reinforced, extrusion, injection molding, improved flowability
Former Lanxess product line is now with Envalior.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Bulk Density
0.800
g/cc
0.0289
lb/in³
ISO 60
Density
1.30
g/cc
0.0470
lb/in³
ISO 1183
Moisture Absorption at Equilibrium
0.20 %
0.20 %
50% RH; ISO 62
Water Absorption at Saturation
0.50 %
0.50 %
ISO 62
Melt Flow
80
g/10 min
@Load 2.16 kg,
Temperature 250 °C
80
g/10 min
@Load 4.76 lb,
Temperature 482 °F
ISO 1133-1
Mechanical Properties
Metric
English
Comments
Tensile Modulus
2.70
GPa
392
ksi
1 mm/min; ISO 527-1,-2
Flexural Yield Strength
75.0
MPa
@Strain 3.5 %
10900
psi
@Strain 3.5 %
2 mm/min; ISO 178-A
Flexural Modulus
2.75
GPa
399
ksi
2 mm/min; ISO 178-A
Flexural Strain at Break
6.0 %
6.0 %
2 mm/min; ISO 178-A
Izod Impact, Notched (ISO)
<=
10.0
kJ/m²
@Temperature 23.0 °C
<=
4.76
ft-lb/in²
@Temperature 73.4 °F
ISO 180-1A
<=
10.0
kJ/m²
@Temperature -30.0 °C
<=
4.76
ft-lb/in²
@Temperature -22.0 °F
ISO 180-1A
<=
10.0
kJ/m²
@Temperature -40.0 °C
<=
4.76
ft-lb/in²
@Temperature -40.0 °F
ISO 180-1A
Izod Impact, Unnotched (ISO)
75.0
kJ/m²
@Temperature -30.0 °C
35.7
ft-lb/in²
@Temperature -22.0 °F
ISO 180-1U
90.0
kJ/m²
@Temperature 23.0 °C
42.8
ft-lb/in²
@Temperature 73.4 °F
ISO 180-1U
Charpy Impact Unnotched
9.00
J/cm²
@Temperature -30.0 °C
42.8
ft-lb/in²
@Temperature -22.0 °F
ISO 179-1eU
13.0
J/cm²
@Temperature 23.0 °C
61.9
ft-lb/in²
@Temperature 73.4 °F
ISO 179-1eU
Charpy Impact, Notched
<=
1.00
J/cm²
@Temperature 23.0 °C
<=
4.76
ft-lb/in²
@Temperature 73.4 °F
ISO 179 1eA
<=
1.00
J/cm²
@Temperature -30.0 °C
<=
4.76
ft-lb/in²
@Temperature -22.0 °F
ISO 179 1eA
Electrical Properties
Metric
English
Comments
Volume Resistivity
>=
1.00e+13
ohm-cm
>=
1.00e+13
ohm-cm
IEC 60093
Surface Resistance
1.00e+15
ohm
1.00e+15
ohm
IEC 60093
Dielectric Constant
3.1
@Frequency 100 Hz
3.1
@Frequency 100 Hz
IEC 60250
3.2
@Frequency 1e+6 Hz
3.2
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor
0.0020
@Frequency 100 Hz
0.0020
@Frequency 100 Hz
IEC 60250
0.019
@Frequency 1e+6 Hz
0.019
@Frequency 1e+6 Hz
IEC 60250
Thermal Properties
Metric
English
Comments
CTE, linear, Parallel to Flow
130
µm/m-°C
@Temperature 23.0 - 55.0 °C
72.2
µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
CTE, linear, Transverse to Flow
130
µm/m-°C
@Temperature 23.0 - 55.0 °C
72.2
µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
Thermal Conductivity
0.250
W/m-K
1.74
BTU-in/hr-ft²-°F
ISO 8302
Melting Point
225
°C
437
°F
10°C/min; ISO 11357-1,-3
Maximum Service Temperature, Air
190
°C
374
°F
IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi)
180
°C
356
°F
ISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi)
60.0
°C
140
°F
ISO 75-1,-2
Vicat Softening Point
170
°C
@Load 5.10 kg
338
°F
@Load 11.2 lb
50°C/h; ISO 306
Flammability, UL94
HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
Oxygen Index
24 %
24 %
Method A; ISO 4589-2
Glow Wire Flammability Index
750
°C
1380
°F
IEC 60695-2-12
Processing Properties
Metric
English
Comments
Melt Temperature
260
°C
500
°F
injection molding; ISO 294
Mold Temperature
80.0
°C
176
°F
injection molding; ISO 294
Drying Temperature
120
°C
248
°F
Dry Time
4.00
-
8.00
hour
4.00
-
8.00
hour
Moisture Content
0.00 - 0.020 %
0.00 - 0.020 %
Karl Fischer
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
BASF Ultradur® B 2550 PBT
Envalior Pocan® DP 1105 000000 PBT
Envalior Pocan® B 1700 000000 PBT
Envalior Pocan® B 1600 000000 PBT
Envalior Pocan® B 1505 Z 000000 PBT
PLANW9185 / 208383
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.