MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient Nymax™ GF 1200 A 40 IM Black 13A Polyamide 66 (Nylon 66)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durability in harsh environments. These materials are available in a broad range of reinforcement levels depending upon stiffness characteristics desired and have been formulated to offer ease of processing in most standard thermoplastic processing equipment

Molded Test Bars: Dry as Molded

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.47 g/cc1.47 g/ccASTM D792
Filler Content 40 %40 %Unspecified
Water Absorption 0.60 %
@Thickness 3.18 mm
0.60 %
@Thickness 0.125 in
@ 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0010 - 0.0035 cm/cm0.0010 - 0.0035 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 187 MPa27100 psiType I, 5.1 mm/min; ASTM D638
Elongation at Break 6.0 %6.0 %Type I, 5.1 mm/min; ASTM D638
Flexural Modulus 11.0 GPa1600 ksiASTM D790
Izod Impact, Notched 1.20 J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
2.25 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
 
Thermal PropertiesMetricEnglishComments
Melting Point 260 °C500 °FASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 246 °C
@Thickness 3.18 mm
475 °F
@Thickness 0.125 in
Unannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Mold Temperature 60.0 - 107 °C140 - 225 °F
Drying Temperature 82.2 °C180 °F
Dry Time 4.00 hour4.00 hour
 
Descriptive Properties
AppearanceBlack
FeaturesGeneral Purpose
 Impact Modified
Filler / ReinforcementGlass Fiber Reinforcement
FormsPellets
Generic MaterialNylon 66
Generic NamePolyamide 66 (Nylon 66)
Processing MethodInjection Molding
Regional AvailabilityNorth America
 South America
UsesAutomotive Applications
 Construction Applications
 Consumer Applications
 General Purpose
 Industrial Applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Nymax™ 1308 A HS Black 13 Polyamide 66 (Nylon 66)
PlastiComp Complet® LCF50 - PA66 Nylon 66, 50% Long Carbon Fiber Reinforced
PlastiComp Complet® LGF50 - PA66 Nylon 66, 50% Long Glass Fiber Reinforced
Ashley Polymers Ashlene® 527LD-14G Nylon 66, 14% Glass Reinforced
Ashley Polymers Ashlene® 527LD-13G Nylon 66, 13% Glass Reinforced

PH0POL1287 / 145856

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.