MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mercury Selenide, HgSe (Tiemannite)
Categories: Ceramic; Sulfide/Chalcogenide; Other Engineering Material; Semiconductor

Key Words: Chalcogenide; Semiconductor; Selenium
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.25 g/cc0.298 lb/in³
a Lattice Constant 6.084 Å6.084 Å
Formula Units/Cell (Z) 44
Molecular Weight 279.55 g/mol279.55 g/mol
 
Mechanical PropertiesMetricEnglishComments
Hardness, Mohs 2.52.5
 
Electrical PropertiesMetricEnglishComments
Band Gap 2.1 eV2.1 eVAlpha Phase
Electron Mobility, cm²/V-s 2000020000
Hole Mobility, cm²/V-s 1.51.5Approximate
 
Thermal PropertiesMetricEnglishComments
CTE, linear 5.46 µm/m-°C
@Temperature 20.0 °C
3.03 µin/in-°F
@Temperature 68.0 °F
Specific Heat Capacity 0.178 J/g-°C0.0425 BTU/lb-°F
Thermal Conductivity 1.00 W/m-K6.94 BTU-in/hr-ft²-°F
Melting Point 797 °C1470 °F
Heat of Formation 247 kJ/mol247 kJ/mol
Debye Temperature -122 °C-188 °F
 
Descriptive Properties
ColorGray
Crystal StructureCubicSphalerite Structure - Space Group F(-4)3m

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mercury Telluride, HgTe (Coloradoite)
Indium Arsenide, InAs
Indium Phosphide, InP
Zinc Selenide, ZnSe
Aluminum Antimonide, AlSb

DSEN22 / 3035

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.