MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polyram RamOfin PPH300G3 Polypropylene, 15% Glass Fiber
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 20% Glass Fiber Filler

Material Notes: 15% Glass fiber reinforced polypropylene for injection molding application.

Information provided by Polyram.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.00 g/cc0.0361 lb/in³ISO 1183
Linear Mold Shrinkage 0.0030 - 0.0070 cm/cm0.0030 - 0.0070 in/inISO 2577
Melt Flow 10 g/10 min
@Load 2.16 kg,
Temperature 230 °C
10 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 65.0 MPa9430 psiISO 527
Elongation at Break 4.0 %4.0 %ISO 527
Tensile Modulus 4.50 GPa653 ksiISO 527
Flexural Strength 90.0 MPa13100 psiISO 178
Flexural Modulus 3.00 GPa435 ksiISO 178
Izod Impact, Notched (ISO) 8.00 kJ/m²3.81 ft-lb/in²ISO 180
 
Thermal PropertiesMetricEnglishComments
Melting Point 165 °C329 °FISO 11357
Maximum Service Temperature, Air 110 °C230 °FContinuous use
 140 °C284 °FShort peaks operation
Deflection Temperature at 0.46 MPa (66 psi) 153 °C307 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 145 °C293 °FISO 75
Flammability, UL94 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Polyram RamOfin PPH300G6 Polypropylene, 30% Glass Fiber
Polyram RamOfin PPH300G9 Polypropylene, 45% Glass Fiber
Polyram RamOfin PPH300G4 Polypropylene, 20% Glass Fiber
Avient Edgetek® PP-15GF/000 Polypropylene (PP), Glass Filled
RheTech Products GC15P200-01 15% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Black

PPOLYR926 / 126723

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.