MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Graft Polymer GRAFTABOND™ EV-MAH 12010 TL Ethylene – Vinyl Acetate copolymer grafted with Maleic Anhydride
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: GRAFTABOND™ EV-MAH 12010 TL is a copolymer of ethylene, so it’s compatible with polyethylene and with most other ethylene copolymers. The vinyl acetate brings flexibility, softness and polarity to the material, and maleic anhydride adds reactive groups to GRAFTABOND™ EV-MAH 12010 TL. This combination of monomers leads to excellent adhesion properties to many different substrates, polar and non-polar alike.

Applications:

  • GRAFTABOND™ EV-MAH 12010 TL is designed for hot melt adhesive formulations
  • It’s compatible with most adhesive resins and waxes
  • Also suitable to produce thermo-adhesive films for solid substrates (PA, PET and PU films, Al foils).
Supplied as: Granulate.

Properties can be regulated to customer needs.

Information provided by Graft Polymer LTD.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Vinyl Acetate Content 28 %28 %By FTIR
Melt Flow 120 g/10 min
@Load 2.16 kg,
Temperature 190 °C
120 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Thermal PropertiesMetricEnglishComments
Melting Point 59.0 °C138 °FISO 11357-3
 
Descriptive Properties
Drying Loss<0.5 g/cc. ASTM D6980. @ 105°C
Maleic Anhydride Graft Level0.5 to 1.3%, FTIR Method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Graft Polymer GRAFTABOND™ ECO 01030 C Polyolefin Based Universal Compatibilizer
Graft Polymer GRAFTABOND™ HD-GMA 02530 C Highly functionalized polyethylene with glycidyl methacrylate
Graft Polymer GRAFTABOND™ HD-MAH 02030 C Highly functionalized polyethylene with maleic anhydride
Graft Polymer GRAFTABOND™ EP-MAH 07110 IM Ethylene-Propylene-Diene-Monomer polymer grafted with Maleic Anhydride
Graft Polymer GRAFTABOND™ LL-PU 01030 C Linear Low Density Polyethylene Functionalized with Isocyanate

PGRAFT932 / 232363

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.