MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

384 Stainless Steel
Categories: Metal; Ferrous Metal; Heat Resisting; Stainless Steel; T 300 Series Stainless Steel

Key Words: UNS S38400, ASTM A493, SAE J405 (30384), 18-8
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.00 g/cc0.289 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 126126before testing
Hardness, Knoop 145145Converted from Brinell
Hardness, Rockwell B 7171Converted from Brinell
Hardness, Vickers 131131Converted from Brinell
Tensile Strength, Ultimate 510 MPa74000 psi
 385 MPa
@Temperature 540 °C
55800 psi
@Temperature 1000 °F
 405 MPa
@Temperature 400 °C
58700 psi
@Temperature 752 °F
 415 MPa
@Temperature 260 °C
60200 psi
@Temperature 500 °F
 470 MPa
@Temperature 120 °C
68200 psi
@Temperature 248 °F
Tensile Strength, Yield 205 MPa
@Strain 0.2 %
29700 psi
@Strain 0.2 %
 145 MPa
@Strain 0.2 %,
Temperature 260 °C
21000 psi
@Strain 0.2 %,
Temperature 500 °F
 145 MPa
@Strain 0.2 %,
Temperature 400 °C
21000 psi
@Strain 0.2 %,
Temperature 752 °F
 170 MPa
@Strain 0.2 %,
Temperature 120 °C
24700 psi
@Strain 0.2 %,
Temperature 248 °F
Elongation at Break 52.5 %52.5 %in 50 mm
 43.2 %
@Temperature 540 °C
43.2 %
@Temperature 1000 °F
in 50 mm
 45.8 %
@Temperature 400 °C
45.8 %
@Temperature 752 °F
in 50 mm
 47.3 %
@Temperature 260 °C
47.3 %
@Temperature 500 °F
in 50 mm
 49.4 %
@Temperature 120 °C
49.4 %
@Temperature 248 °F
in 50 mm
Modulus of Elasticity 193 GPa28000 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000791 ohm-cm
@Temperature 20.0 °C
0.0000791 ohm-cm
@Temperature 68.0 °F
Magnetic Permeability 1.021.02approximate value for the annealed condition at RT
 
Thermal PropertiesMetricEnglishComments
CTE, linear  17.3 µm/m-°C
@Temperature 0.000 - 100 °C
9.61 µin/in-°F
@Temperature 32.0 - 212 °F
 17.8 µm/m-°C
@Temperature 0.000 - 260 °C
9.89 µin/in-°F
@Temperature 32.0 - 500 °F
 18.4 µm/m-°C
@Temperature 0.000 - 540 °C
10.2 µin/in-°F
@Temperature 32.0 - 1000 °F
 18.7 µm/m-°C
@Temperature 0.000 - 650 °C
10.4 µin/in-°F
@Temperature 32.0 - 1200 °F
Specific Heat Capacity 0.500 J/g-°C
@Temperature 0.000 - 100 °C
0.120 BTU/lb-°F
@Temperature 32.0 - 212 °F
Thermal Conductivity  16.3 W/m-K
@Temperature 100 °C
113 BTU-in/hr-ft²-°F
@Temperature 212 °F
 21.5 W/m-K
@Temperature 500 °C
149 BTU-in/hr-ft²-°F
@Temperature 932 °F
Melting Point 1400 - 1455 °C2550 - 2651 °F
Solidus 1400 °C2550 °F
Liquidus 1455 °C2651 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.080 %<= 0.080 %
Chromium, Cr 16 %16 %
Iron, Fe 63 %63 %
Manganese, Mn <= 2.0 %<= 2.0 %
Nickel, Ni 18 %18 %
Phosphorus, P <= 0.045 %<= 0.045 %
Silicon, Si <= 1.0 %<= 1.0 %
Sulfur, S <= 0.030 %<= 0.030 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
410 Stainless Steel
409 Stainless Steel
304 Stainless Steel
301 Stainless Steel
406 Stainless Steel

MQ384C / 12915

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.