MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LATI LATILON 28D M/20 20% Short Glass Fiber Reinforced Polycarbonate (PC)  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, 20% Glass Filled

Material Notes: Description: Latilon thermoplastics are polycarbonate (PC) products. The Latilons feature good mechanical characteristics and excellent toughness even at low temperatures, and good resistance to UV light. Water absorption is low, but a continuous contact with hot water above 50°C is not recommended, as resistance to hydrolysis is not sufficient. Dimensional stability is excellent. Ageing resistance is also very good when the products are free from strains. Reinforced Latilons are among the few polymers to guarantee good mechanical properties also at high temperatures; creep strength is excellent. Continuous no-load working temperature is 135°C (150°C for short periods).

Specific Notes for this Material: UL94 V1 self-extinguishing, bromine and phosphorus free; low fume optical density and toxicity; 20% short glass fibers; good flowability; good surface finish; good impact strength.

Disclaimer from LATI: This document contains information based on average values as obtained from the results of laboratory tests and observations made on LATI materials. Tested materials were injection molded, used in their natural color, and conditioned in compliance with Standard ASTM D 618, procedure A. These values refer to LATI's best technical and scientific knowledge at the moment of testing and cannot be used as a basis for the development of applications. For a better assessment of the materials, you are kindly requested to contact LATI's technical or commercial offices, which are at your disposal and will supply detailed information on the most suitable characteristics for their intended use. With reference to DPR n.224 dated May 24, 1988, issued in accordance with EC Guide-lines 85/374, LATI Industria Termoplastici S.p.A. declines all responsibility arising from an improper use of the products described in this document.

All data provided by LATI.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.34 g/cc0.0484 lb/in³ISO 1183
Water Absorption 0.080 %0.080 %at 23°C; ISO 62
Linear Mold Shrinkage 0.0040 cm/cm0.0040 in/inLATI
Linear Mold Shrinkage, Transverse 0.0040 cm/cm0.0040 in/inLATI
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 9191ASTM D785
Tensile Strength, Ultimate 55.0 MPa7980 psiISO 527
 38.0 MPa
@Temperature 120 °C
5510 psi
@Temperature 248 °F
ISO 527
 43.0 MPa
@Temperature 90.0 °C
6240 psi
@Temperature 194 °F
ISO 527
 45.0 MPa
@Temperature 60.0 °C
6530 psi
@Temperature 140 °F
ISO 527
Flexural Modulus 3.50 GPa508 ksiASTM D790
 3.20 GPa
@Temperature 120 °C
464 ksi
@Temperature 248 °F
ASTM D790
 3.30 GPa
@Temperature 60.0 °C
479 ksi
@Temperature 140 °F
ASTM D790
 3.30 GPa
@Temperature 90.0 °C
479 ksi
@Temperature 194 °F
ASTM D790
Izod Impact, Notched  0.500 J/cm
@Temperature -40.0 °C
0.937 ft-lb/in
@Temperature -40.0 °F
ASTM D256
 0.550 J/cm
@Temperature -20.0 °C
1.03 ft-lb/in
@Temperature -4.00 °F
ASTM D256
 0.700 J/cm
@Temperature 23.0 °C
1.31 ft-lb/in
@Temperature 73.4 °F
ASTM D256
Charpy Impact Unnotched  5.00 J/cm²
@Temperature -20.0 °C
23.8 ft-lb/in²
@Temperature -4.00 °F
DIN 53453
 5.00 J/cm²
@Temperature -40.0 °C
23.8 ft-lb/in²
@Temperature -40.0 °F
DIN 53453
 5.50 J/cm²
@Temperature 23.0 °C
26.2 ft-lb/in²
@Temperature 73.4 °F
DIN 53453
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 22.0 kV/mm
@Thickness 2.00 mm
559 kV/in
@Thickness 0.0787 in
IEC 243-1
Comparative Tracking Index 150 V150 VIEC 112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 30.0 µm/m-°C
@Temperature 20.0 °C
16.7 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Maximum Service Temperature, Air 135 °C275 °F
 150 °C302 °F
Deflection Temperature at 0.46 MPa (66 psi) 143 °C289 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 135 °C275 °FASTM D648
Vicat Softening Point 147 °C297 °F50°C/h 50N; ISO 306
Flammability, UL94  HB
@Thickness 0.710 mm
HB
@Thickness 0.0280 in
 V-2
@Thickness 1.50 mm
V-2
@Thickness 0.0591 in
 V-1
@Thickness 3.00 mm
V-1
@Thickness 0.118 in
Oxygen Index 30 %30 %ISO 4589
 
Processing PropertiesMetricEnglishComments
Melt Temperature 270 - 290 °C518 - 554 °F
Mold Temperature 100 - 120 °C212 - 248 °F
Drying Temperature 120 - 130 °C248 - 266 °FTemperature can be reduced when using vacuum ovens.
Dry Time >= 3 hour>= 3 hourDrying time can be reduced when using vacuum ovens.
 
Descriptive Properties
Heat Resistance - Ball Test (125°C)YIEC 335
Heat Resistance - Ball Test (165°C)NIEC 335
Injection Speedhigh
Needle Burner TestY1.47 mm
 Y3.05 mm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CRP Technology Windform® SP Polyamide-Carbon Fiber Composite for 3D Printing
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
RTP Company RTP 683 HB Acrylonitrile Butadiene Styrene (ABS), Carbon Fiber - UL94 HB
RTP Company RTP 681 HB Acrylonitrile Butadiene Styrene (ABS), Carbon Fiber - UL94 HB
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Sheet

PLATI168 / 50166

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.