MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Wingate Alloys Champaloy Clad Overlay Wear Plate, Chrome Carbide Fusion Plate
Categories: Metal; Ferrous Metal; Alloy Steel; Carbon Steel

Material Notes: Chrome carbide fusion plate

Champaloy is an ultra-hard, impact and abrasion resistant chrome carbide composite alloy formed by metlurgically bonding granular chromium carbide powder to steel. The result is the ultimate wear resistant properties available for the heaviest abrasion/impact applications. The surface of high quality fusion cladding should always contain distribution of large and small stress relief cracks in order to provide maximum wear life in heavily abrasive applications. Stress relief cracks are normal and should occur during the application of fusion cladding to a backing plate. In most applications, proper layout of the stress cracks will provide a wear surface to handle abrasives effectively and economically.

    Advantages:
  • Can be cut, formed and welded
  • Pipe fabricated 2” ID and over
  • Cost effective
  • Stress relieved
  • Extended service life
  • Superior abrasion/impact resistant
  • Good weldability to mild steel base
  • Superior to ceramics
  • Overlay can be applied to two sides for added strength and durability.
Applications: Bucket lips, exhauster blades, hot mill guides, sluce gates, chipper, hoods, fan blades, liner plates, slurry lines, chutes, fan housing, mining equipment, transitions, coal chutes, feeder plates, pipe, truck liners, cone liners, flop gates, scrapers, vibrating pans, cyclones, grizzly bars, shovel liners, wear plates, dozer blades, hoppers, skip cars, whizzer blades.

Information from Wingate Alloys Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 17501750Carbide
Hardness, Rockwell C 6060Matrix
 
Descriptive Properties
Base Plate (in)0.25
Base Plate(in)1.5
Bead Width (in)1.25
Double Pass (in)0.25
 0.375
Single Pass (in)0.1875
 0.25

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Wingate Alloys Winco-Tuf 36 High Strength Wear Plate
Trimay® Wear Plate TWP61 Complex-carbide Flux Cored Weld Wire & Electrode
Trimay® Wear Plate TWP56 Chromium-based Flux Cored Weld Wire & Electrode
Trimay® Wear Plate T170 Nickel-based Steel Overlay
Bisalloy Steels BisPlate HHA Thickness 5-25 mm

NWINGA09 / 122073

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.