MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Akro-Plastic Akromid® B3 GF 50 RM-M (3146) PA 6 Dry, 50% Glass Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 50% Glass Fiber Filled

Material Notes: In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Nevertheless, the viscosity features are on the level of PA6. Especially after storage, e.g. at 150° AKROMID RM shows comparable ageing characteristics. For appliances with very constant features, low warpage, very good finish together with an improved chemical resistance and for production of parts according to the GIT/WIT process, the version B3 GF 30 RM 9 black (3099) or respectively B3 GF 50 9 RM black (3147) offers an ideal solution. However, if a very good impact strength is predominant, our type B3 GF 30 RM black (3016) or respectively B3 GF 50 RM black (3146) will be favored.

High quality surface finish:
B3 GF 30 9 RM black (3099)/B3 GF 50 9 RM black (3147)
Very constant features with regard to climate
Very low warpage
Very good surface
CaCI2 resistant

Cost-effective:
B3 GF 30 RM black (3016)/B3 GF 50 RM black (3146)
Closer to PA 6 GF 30/GF 50
Constant features with regard to climate
Low warpage
Tendentious higher impact strength
Tendentious higher notched impact

Applications:

Electronic market:
e.g. sensor housings, coil former (wo.UL), plug-in connectors, plug panels etc.
Automobile market:
e.g. sensor housing, electrical parts, wind screen wiper bows, door handles, mirror elements, sliding roof frames etc.
General mechanical engineering:
e.g. control elements in printer, copier, housings of valves, pumps etc.

Information from Akro-Plastic

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.62 g/cc0.0585 lb/in³ISO 1183
Filler Content 50 %50 %ISO 1172
Water Absorption 1.2 %
@Temperature 70.0 °C
1.2 %
@Temperature 158 °F
62% RH, Humidity
Linear Mold Shrinkage, Flow 0.0040 cm/cm0.0040 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0070 cm/cm0.0070 in/inISO 294-4
Spiral Flow 50.0 cm19.7 in7 x 4 [mm] diameter
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 280 MPa40600 psiH 961/30; ISO 2039-1
Tensile Strength at Break 210 MPa30500 psi5 [mm/min]; ISO 527-2/5
Elongation at Break 2.2 %2.2 %5 [mm/min]; ISO 527-2/5
Tensile Modulus 17.0 GPa2470 ksi1 [mm/min]; ISO 527-2/1
Flexural Strength 320 MPa46400 psi2 [mm/min]; ISO 178
Flexural Modulus 17.0 GPa2470 ksi2 [mm/min]; ISO 178
Charpy Impact Unnotched  6.00 J/cm²
@Temperature -30.0 °C
28.6 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
 7.00 J/cm²
@Temperature 23.0 °C
33.3 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  1.50 J/cm²
@Temperature -30.0 °C
7.14 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 2.00 J/cm²
@Temperature 23.0 °C
9.52 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 225 °C437 °FDIN EN 11357-1
Deflection Temperature at 1.8 MPa (264 psi) 215 °C419 °FUnannealed; ISO 75-2/A
Deflection Temperature at 8.0 MPa 165 °C329 °FUnannealed; ISO 75-2/C
Flammability, UL94 HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
 
Processing PropertiesMetricEnglishComments
Feed Temperature 60.0 - 80.0 °C140 - 176 °F
Nozzle Temperature 240 - 280 °C464 - 536 °F
Zone 1 225 - 300 °C437 - 572 °F
Zone 2 225 - 300 °C437 - 572 °F
Zone 3 225 - 300 °C437 - 572 °F
Zone 4 225 - 300 °C437 - 572 °F
Melt Temperature 260 - 300 °C500 - 572 °F
Mold Temperature 80.0 - 100 °C176 - 212 °F
Drying Temperature 80.0 °C176 °F
Dry Time 4.00 - 12.0 hour4.00 - 12.0 hour
Hold Pressure 75.0 MPa10900 psi
Back Pressure 5.00 - 10.0 MPa725 - 1450 psi
 
Descriptive Properties
AcetonePass100% Conc
BenzenePass100% Conc
BenzolPass100% Conc
BiodieselPass50°C, 100% Conc
Brake Fluid (DOT4)Fail130°C, 100% Conc
 Pass100% Conc
Calcium chloride, alcoholicFail10% Conc
 Pass10% Conc, when surface treated with 4 (chemical-stabilized)
Calcium chloride, aqueousFail10% Conc
 Pass10% Conc, when surface treated with 4 (chemical-stabilized)
Citric acidPass100% Conc
Diesel fuel (DIN 51601)Pass100% Conc
Sulfuric AcidFail96% Conc
ToluenePass100% Conc
WaterPass100% Conc
Zinc chloride, aqueousFail50% Conc

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Akro-Plastic Akromid® B3 GF 50 1 natural (2531) PA 6 Conditioned, 50% Glass Filled
Akro-Plastic Akromid® B3 GF 50 1 natural (2531) PA 6 Dry, 50% Glass Filled
Akro-Plastic Akromid® B3 GF 50 (2475) PA 6 Dry, 50% Glass Filled
Akro-Plastic Akromid® B3 GF 50 4 RM-M black (3221) PA 6 Dry, 50% Glass Filled
Akro-Plastic Akromid® B3 GF 50 9 RM-M (3147) PA 6 Conditioned, 50% Glass Filled

PAKRO094 / 126874

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.