MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ChevronTexaco Multigear® EP SAE 80W-90
Categories: Fluid; Lubricant

Material Notes: Texaco Multigear EP oils deliver value through:
  • Improved durability — Specially formulated to stand up to the demands of severe service applications.
  • Extended gear life — Extreme pressure properties protect hypoid and other types of gears from scuffing and wear under heavily loaded conditions.
  • Long lubricant life — Outstanding thermal and oxidation stability allow high temperature operation with long lubricant life without the formation of sludge and deposits.
  • All-weather protection — Multiviscosity characteristics assure proper gear lubrication at both low and high ambient temperatures.
  • Corrosion and rust protection — Effective inhibitor package prevents rusting or corrosion of gears and bearings surfaces.

Texaco Multigear EP oils are multipurpose lubricants.

They are made with:

  • Highly refined base stocks
  • A carefully balanced additive package to provide maximum gear protection, long lubricant life and excellent field performance
  • Sulfur-phosphorus extreme pressure additives that provide superior thermal and oxidation stability
  • Rust and corrosion inhibitors, a foam inhibitor, and a pour point depressant

The highly refined base stocks and various inhibitors in the additive package assure a well-balanced lubricant and long gear and bearing life with maximum durability.

Texaco Multigear EP oils are recommended for use in all spiral bevel and hypoid differentials, power dividers, and oil-lubricated steering axle wheel bearings.

They are designed for complete refill and make-up of all passenger car, light duty and heavy duty truck transmissions, conventional differentials and steering gears.

Their multiviscosity characteristics allow their use in equipment operating over a broad ambient temperature range. This means good cold flow properties and gear protection.

Texaco Multigear EP oils meet the performance requirements of:

  • API Service Categories MT-1, GL-4, and GL-5
  • Are qualified for SAE J 2360 (formerly known as MIL-PRF-2105E)

They also meet the requirements of:
  • A Mack GO-J fluid
  • Rockwell 0-76D (SAE 80W-90), 0-76-A (SAE 85W-140)

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

CPS Number: 222316; MSDS Number: 8628

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
API Gravity 28.4 °28.4 °
Brookfield Viscosity 118000 cP
@Temperature -26.0 °C
118000 cP
@Temperature -14.8 °F
Viscosity Measurement 9595Viscosity Index
Saybolt Viscosity at 100°F 762 SUS762 SUS
Saybolt Viscosity at 210°F 76.4 SUS76.4 SUS
Kinematic Viscosity at 40°C (104°F) 145 cSt145 cSt
Kinematic Viscosity at 100°C (212°F) 14.2 cSt14.2 cSt
 
Thermal PropertiesMetricEnglishComments
Pour Point -33.0 °C-27.4 °F
Flash Point 221 °C430 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ChevronTexaco Rando® HDZ 32

WTEXA111 / 76990

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.