MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ineos T00G-00 Polypropylene Impact Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer; Polypropylene, Impact Modified; Molded/Extruded

Material Notes: This is a fractional MFR polypropylene impact copolymer designed for the roofing membrane market. Its blend of impact resistance and flexural modulus is designed to provide an excellent balance between processing and performance. This meets FDA requirements of 21CFR 177.150(c), 3.4.

    Applications
  • Reinforced Roofing membrane

    Benefits
  • Good toughness
  • Flexibility
  • Good MD and TD tear strength
  • Good and consistent processability
  • Wind resistance
  • Good weldability

Information provided by Ineos Olefins & Polymers USA

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.873 g/cc0.0315 lb/in³ASTM D792
Melt Flow 0.60 g/10 min
@Load 2.16 kg,
Temperature 230 °C
0.60 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5252Instantaneous; ASTM D2240
 5252ASTM D785
Tensile Strength at Break 10.8 MPa1560 psi2.0 in/min; ASTM D638
Tensile Strength, Yield 8.48 MPa1230 psi2.0 in/min; ASTM D638
Elongation at Break 620 %620 %2.0 in/min; ASTM D638
Elongation at Yield 38 %38 %2.0 in/min; ASTM D638
Flexural Modulus, 1% Secant 172 MPa25000 psiASTM D790A
Izod Impact, Notched  4.32 J/cm
@Temperature 22.8 °C
8.10 ft-lb/in
@Temperature 73.0 °F
ASTM D256
 7.47 J/cm
@Temperature -20.0 °C
14.0 ft-lb/in
@Temperature -4.00 °F
ASTM D256
Izod Impact, Notched (ISO)  42.4 kJ/m²
@Temperature 22.8 °C
20.2 ft-lb/in²
@Temperature 73.0 °F
Area; ASTM D256
 71.0 kJ/m²
@Temperature -20.0 °C
33.8 ft-lb/in²
@Temperature -4.00 °F
Area; ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 45.6 °C114 °FUnannealed; ASTM D648
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ineos R01C-01 Polypropylene Random Copolymer
Ineos N02G-00 Polypropylene Impact Copolymer
Ineos N20G-00 Polypropylene Impact Copolymer
Ineos R55C-00 Clarified Polypropylene Copolymer
Ineos N00M-00 Polypropylene Impact Copolymer

PINEOS061 / 99382

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.