MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Makrolon® 9125 Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, 20% Glass Filled

Material Notes: MVR (300 °C/1.2 kg) 8.0 cm³/10 min; 20 % glass fiber reinforced; flame retardant; UL 94V-0/1.5 mm; medium viscosity; easy release; injection molding - melt temperature 310 - 330 °C; available in opaque colors only

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Key Words: PC
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.640 g/cc0.0231 lb/in³Pellets; ISO 60
Density 1.34 g/cc0.0484 lb/in³ISO 1183-1
Moisture Absorption at Equilibrium 0.10 %0.10 %50% RH; ISO 62
Water Absorption at Saturation 0.24 %0.24 %ISO 62
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cm0.0030 - 0.0050 in/inparallel/normal; b.o. ISO 2577
Linear Mold Shrinkage, Flow 0.0035 cm/cm0.0035 in/in60x60x2 mm; 500 bar; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0045 cm/cm0.0045 in/in60x60x2 mm; 500 bar; ISO 294-4
Melt Flow 10 g/10 min
@Load 1.20 kg,
Temperature 300 °C
10 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Puncture Resistance  800 N
@Temperature 23.0 °C
180 lb (f)
@Temperature 73.4 °F
ISO 6603-2
 800 N
@Temperature -30.0 °C
180 lb (f)
@Temperature -22.0 °F
ISO 6603-2
Ball Indentation Hardness 148 MPa21500 psiISO 2039-1
Tensile Strength at Break 85.0 MPa12300 psi50 mm/min; ISO 527-1/2
Elongation at Break 2.5 %2.5 %50 mm/min; ISO 527-1/2
Tensile Modulus 5.80 GPa841 ksi1 mm/min; ISO 527-1/2
Flexural Strength 140 MPa20300 psi2 mm/min; ISO 178
Flexural Modulus 5.60 GPa812 ksi2 mm/min; ISO 178
Flexural Strain at Yield 3.0 %3.0 %2 mm/min; ISO 178
Izod Impact, Notched (ISO) 8.00 kJ/m²
@Thickness 3.00 mm
3.81 ft-lb/in²
@Thickness 0.118 in
complete break; ISO 7391/b.o. ISO 180-A
Charpy Impact Unnotched 4.00 J/cm²19.0 ft-lb/in²complete break; ISO 179-1eU
 4.50 J/cm²
@Temperature -30.0 °C
21.4 ft-lb/in²
@Temperature -22.0 °F
complete break; ISO 179-1eU
Charpy Impact, Notched 0.800 J/cm²
@Thickness 3.00 mm
3.81 ft-lb/in²
@Thickness 0.118 in
complete break; ISO 7391/b.o. ISO 179-1eA
Puncture Energy  5.00 J
@Temperature 23.0 °C
3.69 ft-lb
@Temperature 73.4 °F
ISO 6603-2
 5.00 J
@Temperature -30.0 °C
3.69 ft-lb
@Temperature -22.0 °F
ISO 6603-2
Tensile Creep Modulus, 1 hour 5700 MPa827000 psiISO 899-1
Tensile Creep Modulus, 1000 hours 5200 MPa754000 psiISO 899-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmIEC 60093
Surface Resistance 1.00e+16 ohm1.00e+16 ohmIEC 60093
Dielectric Constant  3.3
@Frequency 100 Hz
3.3
@Frequency 100 Hz
IEC 60250
 3.3
@Frequency 1e+6 Hz
3.3
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 36.0 kV/mm914 kV/in1 mm; IEC 60243-1
Dissipation Factor  0.0010
@Frequency 100 Hz
0.0010
@Frequency 100 Hz
IEC 60250
 0.0090
@Frequency 1e+6 Hz
0.0090
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 125 V125 VCTI M; Solution B; IEC 60112
 175 V175 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 30.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
16.7 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
CTE, linear, Transverse to Flow 65.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
36.1 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
Thermal Conductivity 0.230 W/m-K1.60 BTU-in/hr-ft²-°FISO 8302
Hot Ball Pressure Test 136 °C277 °FIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 142 °C288 °FISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 138 °C280 °FISO 75-1,-2
Vicat Softening Point 145 °C293 °F50 N; 50 °C/h; ISO 306
 146 °C295 °F50 N; 120 °C/h; ISO 306
UL RTI, Electrical 130 °C
@Thickness 1.50 mm
266 °F
@Thickness 0.0591 in
UL 746B
UL RTI, Mechanical with Impact 115 °C
@Thickness 1.50 mm
239 °F
@Thickness 0.0591 in
UL 746B
UL RTI, Mechanical without Impact 125 °C
@Thickness 1.50 mm
257 °F
@Thickness 0.0591 in
UL 746B
Flammability, UL94  V-2
@Thickness 0.360 mm
V-2
@Thickness 0.0142 in
 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
Flash Point 470 °C878 °Fignition; ASTM D1929
 550 °C1020 °Fself ignition; ASTM D1929
Oxygen Index 35 %35 %Method A; ISO 4589-2
Glow Wire Ignition Temperature  850 °C
@Thickness 1.50 mm
1560 °F
@Thickness 0.0591 in
IEC 60695-2-13
 850 °C
@Thickness 3.00 mm
1560 °F
@Thickness 0.118 in
IEC 60695-2-13
Glow Wire Flammability Index  960 °C
@Thickness 1.50 mm
1760 °F
@Thickness 0.0591 in
IEC 60695-2-12
 960 °C
@Thickness 3.00 mm
1760 °F
@Thickness 0.118 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Melt Temperature 300 °C572 °FInjection; ISO 294
Mold Temperature 110 °C230 °FInjection; ISO 294
Injection Velocity 200 mm/sec7.87 in/secISO 294
 
Descriptive Properties
Electrolytic corrosionA1IEC 60426
Needle flame test120 sMethod K, 2 mm; IEC 60695-11-5
 120 sMethod K, 3 mm; IEC 60695-11-5
 120 sMethod F, 1.5 mm; IEC 60695-11-5
 120 sMethod F, 2 mm; IEC 60695-11-5
 120 sMethod F, 3 mm; IEC 60695-11-5
 60 sMethod K, 1.5 mm; IEC 60695-11-5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Makrolon® 9425 Polycarbonate
Covestro Makrolon® 2858 Polycarbonate, Injection Grade
Covestro Makrolon® 2458 Polycarbonate, Injection Grade
Mitsubishi Xantar® G4F 23 R Polycarbonate-20% Glass Reinforced
Aluminum 384.0-F Die Casting Alloy

PBA454 / 26955

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.