MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Solvay ALKAMULS® PSML 80 70 LD Surfactant  (discontinued **)
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: ALKAMULS© PSML-80/72 LD is a mild nonionic secondary surfactant, ethoxylated sorbitan ester, that features a very low dioxane content. It Reduces irritancy of baby shampoos and children's bath care products. Good solubilizer for lipohilic substances (petroleum oils, waxes, essential oils) and good emulsification characteristics.

Chemical Name: ETHOXYLATE SORBITAN LAURATE

INCI Name: PEG-80 SORBITAN LAURATE

CAS: 68154-33-6

Available in: Asia Pacific, Europe, Latin America and North America

Applications: ALKAMULS© PSML-80/72 LD is a mild nonionic secondary surfactant, ethoxylated sorbitan ester. Reduces irritancy of baby shampoos and children's bath care products. Good solubilizer for lipohilic substances (petroleum oils, waxes, essential oils) and good emulsification characteristics. ALKAMULS© PSML-80/72 LD features a very low dioxane content. Bath Product, Body Wash, Cream and Body Lotion, Facial Cleanser, Liquid Soap, Shampoo

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Chemical PropertiesMetricEnglishComments
Total Acid Number <= 1.0<= 1.0[meq/g]; RP-0008
 
Optical PropertiesMetricEnglishComments
Gardner Color Number <= 2.0<= 2.0RP-0138
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Component Elements PropertiesMetricEnglishComments
H2O, Water 27 - 30 %27 - 30 %Karl Fisher; RP-0327
 
Descriptive Properties
AppearanceClear to Slightly Hazy Liquid
CompositionDioxane (1,4)<10 ppm, RP-1470
Hydroxyl Number26-30before water, RP-0245
Saponification number7-12 mg KOH/gRP-0496

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Low Density Polyethylene (LDPE), Extrusion Grade
Overview of materials for Linear Low Density Polyethylene (LLDPE), Extrusion Grade
Overview of materials for High Density Polyethylene (HDPE), Extruded
ChevronTexaco Snow White Petrolatum

WRHOD047 / 137277

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.