MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Kingfa PA6-G15 15% Glass Fiber Reinforced PA6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 20% Glass Fiber Filled

Material Notes:
    Features:
  • Good size stability
  • Low tendency to wrap
  • High mechanical properties
  • Good low temperature resistance
  • Good surface
  • Excellent balance properties

    Applications:
  • Injection molding
  • Automobile parts
  • Power tools
  • Machinery parts
  • Sport appliance

Information Provided by Kingfa Sci. & Tech. Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.24 g/cc
@Temperature 23.0 °C
1.24 g/cc
@Temperature 73.4 °F
ASTM D792
Filler Content 15 %15 %Glass Fiber
Water Absorption 0.60 %
@Temperature 23.0 °C,
Time 86400 sec
0.60 %
@Temperature 73.4 °F,
Time 24.0 hour
ASTM D570
Linear Mold Shrinkage 0.0060 - 0.012 cm/cm
@Temperature 23.0 °C
0.0060 - 0.012 in/in
@Temperature 73.4 °F
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 119119ASTM D785
Tensile Strength at Break 125 MPa18100 psi10mm/min; ASTM D638
Elongation at Break 4.1 %4.1 %10mm/min; ASTM D638
Flexural Strength 175 MPa25400 psi2mm/min; ASTM D790
Flexural Modulus 5.76 GPa835 ksi2mm/min; ASTM D790
Izod Impact, Notched 0.950 J/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
1.78 ft-lb/in
@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmASTM D257
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 215 °C
@Thickness 6.40 mm
419 °F
@Thickness 0.252 in
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 207 °C
@Thickness 6.40 mm
405 °F
@Thickness 0.252 in
ASTM D648
Flammability, UL94  HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature <= 300 °C<= 572 °F
Rear Barrel Temperature 225 - 245 °C437 - 473 °FStart Point: 230°C
Middle Barrel Temperature 250 - 270 °C482 - 518 °FStart Point: 255°C
Front Barrel Temperature 260 - 280 °C500 - 536 °FStart Point: 265°C
Melt Temperature 255 - 285 °C491 - 545 °FStart Point: 265°C
Mold Temperature 50.0 - 70.0 °C122 - 158 °FStart Point: 60°C
Drying Temperature 90.0 - 110 °C
@Time 14400 - 21600 sec
194 - 230 °F
@Time 4.00 - 6.00 hour
Pre-dry
 
Descriptive Properties
Injection SpeedModerate to High

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kingfa PA6-G50 50% Glass Fiber Reinforced PA6
Avient Bergamid™ A70 G15 HW TM-Z Polyamide 66 (Nylon 66)
Asahi Kasei Leona™ 90G50 Polyamide 66, GF Reinforced
Envalior Akulon® K224-G6U PA6-GF33, Conditioned, 33% Glass Filled
Envalior Akulon® K224-G6U PA6-GF33, Dry, 33% Glass Filled

PKINGF020 / 104279

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.