MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M Scotchcal™ ElectroCut™ 404 Graphic Film
Categories: Polymer; Film

Material Notes: Product Description:
  • 3.25 mil cast film in 6 glossy, opaque, fluorescent color
  • Extremely conspicuous in daylight and activated by exposure to near ultraviolet light (but not black light)
  • Offers high attention value under poor visibility, particularly at dawn or dusk
  • Good electronic cutting characteristics as small as 12 mm tall
  • Printable with solvent-based screen print inks
  • Good weather resistance

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 82.5 microns3.25 milwithout adhesive
 102 microns4.00 milwith adhesive
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break >= 8.62 MPa>= 1250 psi
Peel Strength 0.701 kN/m4.00 pliAdhesion to Acrylic
 0.701 kN/m4.00 pliAdhesion to Glass
 0.701 kN/m4.00 pliAdhesion to Polycarbonate
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 107 °C225 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
 
Descriptive Properties
AppearanceYellow Orange

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M 927 Adhesive Transfer Tapes with Adhesive 300
3M FM142 Indoor UL Recognized Computer Imprintable Clear Polyester Label Product
3M 6035PC 12026 Polyurethane Foam Tape
3M 467MP High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M 7225 HP Indigo Optimized Polyester Label Product

PMM35322 / 170069

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.