MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ELASTO UK Dryflex® 660700S SEBS Based Material, Semi-Filled Qualities, 70A Hardness, Natural
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes: The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine the advantages of the other two series. The material has good flow and mechanical properties as well as reasonable scratch resistance.

Information from Vita Thermoplastic Polymers (VTP).

Vita Thermoplastic Polymers was aquired by HEXPOL and is now ELASTO

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.05 g/cc1.05 g/ccASTM D792
Linear Mold Shrinkage 0.0080 - 0.020 cm/cm0.0080 - 0.020 in/in
Melt Flow 5.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
5.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 70
@Thickness 4.00 mm
70
@Thickness 0.157 in
ASTM D2240
Tensile Strength at Break 8.00 MPa1160 psiASTM D638
Elongation at Break >= 600 %>= 600 %ASTM D638
100% Modulus 3.00 MPa
@Strain 100 %
435 psi
@Strain 100 %
ASTM D638
300% Modulus 4.00 MPa
@Strain 300 %
580 psi
@Strain 300 %
ASTM D638
Tear Strength 29.0 kN/m165 pliASTM D624
Compression Set 25 %
@Temperature 23.0 °C,
Time 259000 sec
25 %
@Temperature 73.4 °F,
Time 72.0 hour
ASTM D395
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 125 °C257 °F
Minimum Service Temperature, Air -50.0 °C-58.0 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 180 - 210 °C356 - 410 °F
 
Descriptive Properties
Bonding to PPExcellent
Chemical ResistanceGoodExcluding organic solvents, aromatic and vegetable oils
ColorNatural
Weather ResistanceExcellentAir ageing

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company RTP 2700 S-80A Z Saturated Styrenic Block Copolymer (TES/SEBS or other), FDA Compliant Ingredients
Radici Heraflex® A 80-21-94 TPS-SEBS Thermoplastic Elastomer
Kraton® G4609 H (SEBS) with Oil
ELASTO UK Dryflex® 600700S SEBS Based Material, Filled Qualities, 70A Hardness, Natural
Dynasol Calprene® H6171 Hydrogenated Rubber (SEBS)

PVTC104 / 72173

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.