MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Azoty Tarnow™ Tarnamid® T-27 GF10 MX10 Polyamide 6 - Flame Retarded, Reinforced  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Glass Fiber Filled, Flame Retardant

Material Notes: Flame retarded grade, reinforced with 10% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning, good surface quality.

Tarnamid® has the following main properties:

  • High mechanical strength, rigidity and hardness
  • High impact strength
  • High vibration damping capacity
  • Good fatigue strength
  • Very good sliding properties, abrasion resistance, low coefficient of friction
  • High thermal resistance, admissible temperature of continuous operation from -60°C to +150°C
  • High chemical resistance, particularly to organic solvents, oils, lubricants and fuels
  • Considerable moisture absorption influencing mechanical and electrical properties
  • Self-extinguishing properties (fire retardant properties)
  • Good electro-insulating properties
  • Good optical properties, relatively good transparency of molded pieces with thickness below 3.2 mm made from natural Tarnamid® (not dyed and not compounded)
  • Can be used for the production of goods coming into contact with food (grades fulfilling requirement of European Union Directive No 2002/72/EEC) with latest amendments

Information provided by Azoty Tarnow™.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.62 g/cc1.62 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.0040 cm/cm0.0040 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0080 cm/cm0.0080 in/inISO 294-4
Melt Flow 10 g/10 min
@Load 5.00 kg,
Temperature 275 °C
10 g/10 min
@Load 11.0 lb,
Temperature 527 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness  200 MPa
@Load 36.5 kg
29000 psi
@Load 80.5 lb
cond.; ISO 2039-1
 370 MPa
@Load 36.5 kg
53700 psi
@Load 80.5 lb
dry; ISO 2039-1
Tensile Strength 78.0 MPa11300 psicond.; ISO 527
 105 MPa15200 psidry; ISO 527
Elongation at Break 3.0 %3.0 %dry; ISO 527
 4.0 %4.0 %cond.; ISO 527
Tensile Modulus 6.70 GPa972 ksicond.; ISO 527
 10.3 GPa1490 ksidry; ISO 527
Flexural Strength 120 MPa17400 psicond.; ISO 178
 170 MPa24700 psidry; ISO 178
Charpy Impact Unnotched 3.00 J/cm²14.3 ft-lb/in²dry; ISO 179 1eU
 4.00 J/cm²19.0 ft-lb/in²cond.; ISO 179 1eU
Charpy Impact, Notched 0.350 J/cm²1.67 ft-lb/in²dry; ISO 179 1eA
 0.400 J/cm²1.90 ft-lb/in²cond.; ISO 179 1eA
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 1.00e+15 ohm1.00e+15 ohmIEC 93
Dielectric Strength 28.0 kV/mm711 kV/inIEC 243-1
Comparative Tracking Index 600 V600 VIEC 112
 
Thermal PropertiesMetricEnglishComments
Melting Point 221 °C430 °F
Deflection Temperature at 1.8 MPa (264 psi) 130 °C266 °Fcond.; ISO 75
 160 °C320 °Fdry; ISO 75
Vicat Softening Point  200 °C
@Load 5.10 kg
392 °F
@Load 11.2 lb
cond.; ISO 306
 210 °C
@Load 5.10 kg
410 °F
@Load 11.2 lb
dry; ISO 306
Minimum Service Temperature, Air -60.0 °C-76.0 °F
Flammability, UL94 V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
Glow Wire Flammability Index 960 °C
@Thickness 2.00 mm
1760 °F
@Thickness 0.0787 in
PN-EN-60695-2-12
 
Processing PropertiesMetricEnglishComments
Melt Temperature 230 - 290 °C446 - 554 °F
Mold Temperature 60.0 - 120 °C140 - 248 °F80 - 90°C is recommended
Drying Temperature 75.0 - 100 °C
@Time 7200 - 14400 sec
167 - 212 °F
@Time 2.00 - 4.00 hour
Moisture Content <= 0.10 %<= 0.10 %
Injection Pressure 80.0 - 130 MPa11600 - 18900 psi80 MPa is recommended

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Azoty Tarnow™ Tarnamid® T-27 GF10 MX6 Polyamide 6 - Flame Retarded, Reinforced
Azoty Tarnow™ Tarnamid® T-27 GF15 Polyamide 6 - Glass Fiber Reinforced
Lehvoss LUVOCOM® 1-8181 Polyamide 66 with carbon fiber, toughness-modified
Azoty Tarnow™ Tarnamid® T-27 GF15 FRV0 Polyamide 6 - Flame Retarded, Reinforced
Polymer Resources NY66-IMG13 Nylon, 13% Glass Reinforced, Impact Modified (DAM)

PZAK926 / 121878

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.