MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chemours Viton® GBL-900 Fluoroelastomer (FKM)  (discontinued **)
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: Gum polymer (curative not incorporated). Excellent resistance to automotive lubricating oils, aqueous fluids

Temperature of Retraction (TR-10): -15°C. Polymer Fluorine Content: 67%. Volume Increase After 7 Days/Methanol/23°C: 40 to 50%

Applications: Compression molding automotive lubricating oil, coolant system seals.

Viton Type B Information: Comprised of vinylidene fluoride (VF2), hexafluoroproylene (HFP) and tetrafluoroethylene (TFE). Middle fluorine content of Viton standard grades leads to medium chemical resistance and flexibility at low temperatures.

General Viton Information: Viton was introduced in 1957 as a high-performance aerospace sealing elastomer. It is now also used in other industries including automotive, fluid power, appliance, and chemical industries. It is noted for its outstanding performance in very hot and extremely corrosive environments. Compounds of Viton remain elastic indefinitely at 204°C or when exposed intermittently to 260°C under laboratory conditions. Viton is generally serviceable down to -18 to -23°C, although special formulations permit static use down to -54°C (-65°F). Also, Viton has proven to be satisfactory for static seals under conditions approaching absolute zero. Viton has excellent resistance to oils, fuels, lubricants, and most mineral acids. It has extremely low permeability to a broad range of substances. It is resistant to aliphatic, aromatic hydrocarbons. It is extremely resistant to compression set, even at high temperatures. It has exceptional good resistance to atmospheric oxidation, sun, weather, fungus, and mold. It has good electrical properties in low voltage, low frequency applications and low burning characteristics.

Information provided by DuPont Dow Elastomers.

Chemours was formed from former DuPont performance chemicals businesses, including the Viton product line, in 2015. This specific grade had been discontinued prior to the spinoff.

Key Words: Rubbers
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.85 g/cc0.0668 lb/in³
Mooney Viscosity 90
@Temperature 121 °C
90
@Temperature 250 °F
Nominal Viscosity, ML 1+10
 
Mechanical PropertiesMetricEnglishComments
Compression Set 35 %
@Temperature 200 °C
35 %
@Temperature 392 °F
70 hours
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 204 °C399 °FContinuous use
 >= 260 °C>= 500 °FIntermittent use
Minimum Service Temperature, Air -23.0 - -18.0 °C-9.40 - -0.400 °FViton is generally useful down to -18 to -23°C.
 
Component Elements PropertiesMetricEnglishComments
Fluorine, F 67 %67 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chemours Viton® A-201C Fluoroelastomer (FKM)
Chemours Viton® A-HV Fluoroelastomer (FKM)
Chemours Viton® B-601C Fluoroelastomer (FKM)
Chemours Viton® B-435C Fluoroelastomer (FKM)
Chemours Viton® GBLT-600S Fluoroelastomer Compound

PDVD48 / 33918

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.