MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Röhm CYROLITE R30 Acrylic-Based Multipolymer Compound  (discontinued **)
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Impact Modified, Molded

Material Notes:

Information Provided by Evonik CYRO. The former Evonik Methacrylates business has been sold to Röhm (Roehm) GmbH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.07 g/cc1.07 g/ccASTM D792
Bulk Density 0.660 g/cc0.0238 lb/in³ASTM D1895
Water Absorption <= 0.30 %<= 0.30 %ASTM D570
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm0.0040 - 0.0070 in/inASTM D951
Melt Flow 6.0 g/10 min
@Load 5.00 kg,
Temperature 230 °C
6.0 g/10 min
@Load 11.0 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell L 4747ASTM D785
Tensile Strength at Break 37.9 MPa5500 psiASTM D638
Elongation at Break 22 %22 %ASTM D638
Elongation at Yield 4.2 %4.2 %ASTM D638
Tensile Modulus 1.65 GPa240 ksiASTM D638
Flexural Strength 61.4 MPa8900 psiASTM D790
Flexural Modulus 1.59 GPa230 ksiASTM D790
Izod Impact, Notched 0.747 J/cm
@Diameter 6.35 mm
1.40 ft-lb/in
@Diameter 0.250 in
BAR; ASTM D256
 0.641 J/cm
@Diameter 6.35 mm,
Temperature 0.000 °C
1.20 ft-lb/in
@Diameter 0.250 in,
Temperature 32.0 °F
BAR; ASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear 72.0 µm/m-°C
@Temperature 0.000 - 100 °C
40.0 µin/in-°F
@Temperature 32.0 - 212 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 81.1 °C
@Thickness 6.35 mm
178 °F
@Thickness 0.250 in
Annealed; ASTM D648
Vicat Softening Point 97.2 °C207 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.521.52ASTM D542
Haze 2.0 %2.0 %ASTM D1003
Yellow Index -1.50 %-1.50 %ASTM E313
Transmission, Visible 88 %88 %ASTM D1003
 
Processing PropertiesMetricEnglishComments
Middle Barrel Temperature 193 - 246 °C380 - 475 °FCylinder Temp
Melt Temperature 204 - 246 °C400 - 475 °F
Mold Temperature 32.2 - 65.6 °C90.0 - 150 °F
Drying Temperature 79.4 °C175 °F
Dry Time 3 - 4 hour3 - 4 hour

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Americas Styrenics STYRON® 666D High Heat Crystal Polystyrene
Celanese CoolPoly® E1201 Thermally Conductive Polypropylene
Röhm CYROLITE G-20 Acrylic-Based Multipolymer Molding Compound
Röhm CYROLITE CG-97 Acrylic-Based Multipolymer Compound
Evonik CYROLITE CYROVU HP2 Acrylic-Based Multipolymer Compound

PCYR00034 / 89038

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.