MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

ExxonMobil Exxon™ IT0316 Ethylene Propylene Copolymer Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Exxon IT0316 is an elastic ethylene propylene copolymer processing additive for use in EPDM formulations. It improves flow in extrusion dies and increases extrusion speed with minimal effect on properties when used at 10 phr. It can also be utilized in butyl/EPDM formulations designed for use in inner tubes, increasing tack and green strength.

Key Features:

  • Improves extrusion speed.
  • Maintains properties at up to 10 phr.
  • Works in EPDM hose, profile and inner tube formulations.
  • Free flowing pellets.
Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South America

Information provided by ExxonMobil Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Mooney Viscosity 22
@Temperature 125 °C
22
@Temperature 257 °F
ML(1+4), Radial cavity dies, polymer remassed at 145±°C; ASTM D1646
 
Descriptive Properties
Ethylene Content16 %ASTM D3900

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Vistalon™ 878P Ethylene Propylene Copolymer Rubber
Shandong Dongyue Shenzhou New Material Co DS602 Perfluorinated Ethylene-Propylene Copolymer
Shandong Dongyue Shenzhou New Material Co DS601 Perfluorinated Ethylene-Propylene Copolymer
Shandong Dongyue Shenzhou New Material Co DS600 Perfluorinated Ethylene-Propylene Copolymer
Overview of materials for EMAAA Terpolymer

PEXA928a / 140755

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.