MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Nanocyl PLASTICYL™ SEBS1001 SEBS (styrene-ethylene/butadiene-styrene) with 10% Multi-Wall Carbon Nanotubes
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene/Butadiene/Styrene (SBS)

Material Notes: PLASTICYL™ is a family of Multi-Wall Carbon Nanotube (MWNT) thermoplastic concentrates for applications requiring superior electrical conductivity and electrostatic discharge (ESD) properties. PLASTICYL™ SEBS1001 is a conductive masterbatch based on SEBS (styrene-ethylene/butadiene-styrene) with 10% NC7000.

Key Applications: Masterbatch for the production of SEBS and SBS antistatic materials or wasting electrostatic for injection molding

Suggested Dilution: The suggested dilution for this product is dependent on the desired characteristics of resistivity, which are closely related to molding settings. In order to find the appropriate dilution we strongly recommend performing tests at different percentages in working conditions.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Filler Content 10 %10 %Carbon Nanotube Loading
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.5 ohm-cm2.5 ohm-cmISO 3915

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Techmer ES Electrablend® PPS 06000
Parker Chomerics Tecknit SC-Consil® 860 Carbon-Filled Silicone Elastomer
NuSil SCV-2596 Silicone, Ultralow Outgassing™
Celanese Celstran® PA66-SF10-02 PA66, 10% Stainless Steel Reinforced
BASF Ultrason® E 2010 C6 30% Carbon Filled

PNANOCY988 / 108943

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.