Turco C NVT is a heavy-duty, alkaline cleaner for immersion and barrel cleaning operations. It is particularly suited to plating, porcelain enameling and other critical finishing operations which require the utmost in cleanliness. In addition, it has soil tolerance, and cleans and rinses well even under the heavy soil loads of barrel washing of screw and header machine products.Applications:- Alkaline Cleaning
- Magnesium Phosphate Conversion Coatings
- Zinc Phosphate Conversion Coatings
|
Aerospace Surface Treatment |