MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

Alcoa Excalibar® 6013-T8 Aluminum, 0.3-1.9 cm diameter
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 6000 Series Aluminum Alloy

Material Notes: Weldability = A; Stress Corrosion Cracking Resistance = A; General Corrosion Resistance = B (A = best; E = worst). General 6013 characteristics and uses: High strength and good corrosion resistance. Easily joined by all welding and brazing methods. Excellent compressive properties. Good applied coating acceptance and good machinability.

Uses: ABS Braking systems, hydraulic applications, valves, machine parts, roller blade parts, munitions.

Data supplied by the manufacturer, Alcoa.

Key Words: Aluminum 6013-T8; 6013-T8 Aluminium; Alcoa, Aluminum Company of America; AA6013-T8; UNS A96013
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.71 g/cc0.0979 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 130130500 kg load/10 mm ball
Hardness, Knoop 163163Estimated from Brinell
Hardness, Rockwell A 49.549.5Estimated from Brinell
Hardness, Rockwell B 8080Estimated from Brinell
Hardness, Vickers 149149Estimated from Brinell
Tensile Strength, Ultimate >= 413 MPa>= 59900 psi
Tensile Strength, Yield >= 392 MPa>= 56900 psi
Elongation at Break 5.0 %5.0 %in 5 cm.
Modulus of Elasticity 69.6 GPa10100 ksi
Machinability 70 %70 %0-100 Scale (A=90; B=70; C=50; D=30; E=10)
Shear Strength 246 MPa35700 psiCalculated
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000450 ohm-cm0.00000450 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 23.4 µm/m-°C
@Temperature 20.0 - 100 °C
13.0 µin/in-°F
@Temperature 68.0 - 212 °F
average
Thermal Conductivity 164 W/m-K1140 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 97 %97 %
Chromium, Cr <= 0.10 %<= 0.10 %
Copper, Cu 0.60 - 1.1 %0.60 - 1.1 %
Iron, Fe <= 0.50 %<= 0.50 %
Magnesium, Mg 0.80 - 1.2 %0.80 - 1.2 %
Manganese, Mn 0.20 - 0.80 %0.20 - 0.80 %
Silicon, Si 0.60 - 1.0 %0.60 - 1.0 %
Titanium, Ti <= 0.10 %<= 0.10 %
Zinc, Zn <= 0.25 %<= 0.25 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 5154-O
Aluminum 5154-H112
6082-O Aluminum
6111 Aluminum Composition Spec
6022 Aluminum Composition Spec

NALCOA11 / 14746

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.