MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M Techical Ceramics Ekasic® P Silicon Carbide
Categories: Ceramic; Carbide

Material Notes:

Information provided by 3M Technical Ceramics, formerly ESK Ceramics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.76 - 2.89 g/cc0.0997 - 0.104 lb/in³DIN EN 623-2
Porosity 10 - 14 %10 - 14 %DIN EN 623-2
Grain Size <= 5.0 µm<= 5.0 µm
Weibull Modulus 1515[m]; DIN EN 843-5
 
Mechanical PropertiesMetricEnglishComments
Hardness, Knoop 24
@Pressure 100 MPa
24
@Pressure 14500 psi
DIN EN 843-4
Hardness, Vickers 24.5
@Pressure 1000 MPa
24.5
@Pressure 145000 psi
DIN EN 843-4
Tensile Modulus 340 GPa49300 ksiYoung's; DIN EN 843-2
Flexural Strength 225 MPa32600 psi4-pt bending; DIN EN 843-1
Compressive Strength >= 2000 MPa>= 290000 psiDIN 51104
Poissons Ratio 0.130.13DIN EN 843-2
Fracture Toughness 3.00 MPa-m½2.73 ksi-in½SENB
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 1.00e+8 ohm-cm>= 1.00e+8 ohm-cmDIN EN 50359
 
Thermal PropertiesMetricEnglishComments
CTE, linear  3.80 µm/m-°C
@Temperature 25.0 - 500 °C
2.11 µin/in-°F
@Temperature 77.0 - 932 °F
DIN EN 821-1
 5.10 µm/m-°C
@Temperature 500 - 1000 °C
2.83 µin/in-°F
@Temperature 932 - 1830 °F
DIN EN 821-1
Specific Heat Capacity 0.690 J/g-°C0.165 BTU/lb-°FC DIN EN 821-3
Thermal Conductivity 110 W/m-K763 BTU-in/hr-ft²-°FDIN EN 821-2
 
Descriptive Properties
Thermal Stress152 KR1 = sB·(1-ν)/(α·E)
 17 W/mmR2= R1-λ

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CoorsTek UltraSiC™ SC-30 Direct Sintered Silicon Carbide
Morgan Advanced Ceramics CVD Silicon Carbide
CoorsTek Nitrogen Bonded Silicon Carbide, SCNB
Schunk CarSIK CT Silicon Carbide
Silicon Carbide, Reaction-Bonded, SiSiC

CESK09 / 183301

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.