MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M Scotch-Weld™ 826 Nitrile Rubber & Plastic Adhesive
Categories: Polymer; Adhesive

Material Notes:

Features:

  • A light colored, fast drying adhesive
  • Excellent resistance to aromatic fuels, water and oil
  • Used to bond many types of plastic films including ABS, cellulose acetate, and PVC

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 21 - 25 %21 - 25 %
Brookfield Viscosity 750 - 1250 cP750 - 1250 cPRVF #2 sp @ 20 rpm @ 27°C
 
Mechanical PropertiesMetricEnglishComments
Shear Strength  0.172 MPa
@Temperature 121 °C
25.0 psi
@Temperature 250 °F
Overlap, Alum/Alum
 0.379 MPa
@Temperature 93.0 °C
55.0 psi
@Temperature 199 °F
Overlap, Alum/Alum
 0.386 MPa
@Temperature 82.0 °C
56.0 psi
@Temperature 180 °F
Overlap, Alum/Alum
 0.607 MPa
@Temperature 66.0 °C
88.0 psi
@Temperature 151 °F
Overlap, Alum/Alum
 1.37 MPa
@Temperature 24.0 °C
198 psi
@Temperature 75.2 °F
Overlap, Alum/Alum
 9.618 MPa
@Temperature -55.0 °C
1395 psi
@Temperature -67.0 °F
Overlap, Alum/Alum
 12.49 MPa
@Temperature -34.0 °C
1811 psi
@Temperature -29.2 °F
Overlap, Alum/Alum
Peel Strength  0.701 kN/m
@Temperature 82.0 °C
4.00 pli
@Temperature 180 °F
180°, Canvas/Steel
 0.877 kN/m
@Temperature 66.0 °C
5.00 pli
@Temperature 151 °F
180°, Canvas/Steel
 1.75 kN/m
@Temperature 24.0 °C
10.0 pli
@Temperature 75.2 °F
180°, Canvas/Steel
 2.98 kN/m
@Temperature 24.0 °C
17.0 pli
@Temperature 75.2 °F
180°, Canvas/Steel
 3.07 kN/m
@Temperature -34.0 °C
17.5 pli
@Temperature -29.2 °F
180°, Canvas/Steel
 3.24 kN/m
@Temperature 24.0 °C
18.5 pli
@Temperature 75.2 °F
180°, Canvas/Steel
 3.68 kN/m
@Temperature 24.0 °C
21.0 pli
@Temperature 75.2 °F
180°, Canvas/Steel
 4.03 kN/m
@Temperature 24.0 °C
23.0 pli
@Temperature 75.2 °F
180°, Canvas/Steel
 4.73 kN/m
@Temperature 24.0 °C
27.0 pli
@Temperature 75.2 °F
180°, Canvas/Steel
 1.58 kN/m
@Temperature 49.0 °C,
Time 86400 sec
9.00 pli
@Temperature 120 °F,
Time 24.0 hour
T-Peel, Canvas/Canvas, aged 2 days @ 49°C, Jet Fuel
 2.80 kN/m
@Temperature 49.0 °C,
Time 86400 sec
16.0 pli
@Temperature 120 °F,
Time 24.0 hour
T-Peel, Canvas/Canvas, aged 2 days @ 49°C, VMP
 3.68 kN/m
@Temperature 49.0 °C,
Time 86400 sec
21.0 pli
@Temperature 120 °F,
Time 24.0 hour
T-Peel, Canvas/Canvas, aged 2 days @ 49°C, Oil
 2.10 kN/m
@Time 1.21e+6 sec
12.0 pli
@Time 336 hour
T-Peel, Canvas/Canvas, aged 2 days @ 49°C, Freon #11
 2.28 kN/m
@Time 605000 sec
13.0 pli
@Time 168 hour
T-Peel, Canvas/Canvas, aged 2 days @ 49°C, Freon #11
 2.63 kN/m
@Time 605000 sec
15.0 pli
@Time 168 hour
T-Peel, Canvas/Canvas, aged 2 days @ 49°C, Freon #12
 2.63 kN/m
@Time 1.21e+6 sec
15.0 pli
@Time 336 hour
T-Peel, Canvas/Canvas, aged 2 days @ 49°C, Freon #12
 
Thermal PropertiesMetricEnglishComments
Flash Point 2.00 °C35.6 °FSetaflash
 
Processing PropertiesMetricEnglishComments
Shelf Life 15.0 Month15.0 Month
 
Descriptive Properties
AppearanceLight Amber
BaseNitrile

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lord Adhesives HPC-5B Hydrogenated Nitrile Butadiene Rubber Coating
3M Scotch-Weld™ 4491 Nitrile Industrial Adhesive
3M Scotch-Weld™ 1099-L Nitrile High Performance Plastic Adhesives
3M Scotch-Weld™ 1099 Nitrile High Performance Plastic Adhesives
Lord Adhesives HPC-5C Hydrogenated Nitrile Butadiene Rubber Coating

PMM34123 / 168870

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.