MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Borealis BC650MO Polypropylene Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: BC650MO is a very high impact polypropylene heterophasic copolymer intended for injection molding. This product offers a good UV resistance, further enhanced by pigmentation. This grade features high impact strength, high thermal stability and very good processability. As all polypropylenes, this grade shows excellent stresscracking and chemical resistances. This grade is characterized by combination of good stiffness, good creep resistance and very high impact strength even at low temperatures. This grade is mildly nucleated to maximize the mechanical stiffness. The additive formulation provides a smooth demolding. Nucleation, good flow properties and high stiffness create a high potential for cycle time reduction. Its very good organoleptic properties allows this grade to be used with any masterbatch without discoloring problems. Applications: crates and boxes, pallets, technical parts, bottle trays, and luggage.

Information provided by Borealis AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.904 g/cc0.0327 lb/in³ISO 1183
Linear Mold Shrinkage 0.010 - 0.020 cm/cm0.010 - 0.020 in/in
Melt Flow 4.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
4.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 8080ISO 2039-2
Tensile Strength, Yield 22.5 MPa3260 psi50mm/min; ISO 527-2
Elongation at Yield 5.5 %5.5 %50mm/min; ISO 527-2
Tensile Modulus 1.20 GPa174 ksi1mm/min; ISO 527-2
Charpy Impact, Notched  0.750 J/cm²
@Temperature -20.0 °C
3.57 ft-lb/in²
@Temperature -4.00 °F
ISO 179/1eA
 2.00 J/cm²
@Temperature 23.0 °C
9.52 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
Puncture Energy  41.0 J
@Temperature -40.0 °C
30.2 ft-lb
@Temperature -40.0 °F
ISO 6603-2
 46.0 J
@Temperature -20.0 °C
33.9 ft-lb
@Temperature -4.00 °F
ISO 6603-2
 48.0 J
@Temperature 0.000 °C
35.4 ft-lb
@Temperature 32.0 °F
ISO 6603-2
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C194 °FISO 75-2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 230 - 260 °C446 - 500 °F
Mold Temperature 10.0 - 30.0 °C50.0 - 86.0 °F
Hold Pressure 20.0 - 50.0 MPa2900 - 7250 psi
 
Descriptive Properties
Injection Velocityhighest possible

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis BC612WG Polypropylene Copolymer
Borealis BC142MO Polypropylene Copolymer
Borealis Borpact™ BC914TF Polypropylene Copolymer
Borealis BC545MO Polypropylene Copolymer
Borealis BC918CF Polypropylene Copolymer

PBOREA312 / 108572

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.