MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Borealis Borclear™ RB709CF Polypropylene Ethylene Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Borclear™ RB709CF is a propylene -ethylene copolymer. This grade is suitable for the manufacturing of unoriented film on blown film lines. Applications: Borclear™ RB709CF is recommended for sealing layer in co extrusion, food packaging, lamination films, and additives. Borclear RB709CF is slip and antiblock free

Information provided by Borealis AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 - 0.910 g/cc0.0325 - 0.0329 lb/in³ISO 1183
Melt Flow 1.5 g/10 min
@Load 2.16 kg,
Temperature 230 °C
1.5 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 550 - 600 %550 - 600 %MD/TD; ISO 527-3
Tensile Modulus 0.730 GPa106 ksiMD/TD; ISO 527-3
Flexural Modulus 0.650 GPa94.3 ksiISO 178
Dart Drop, Total Energy 50.0 J36.9 ft-lbISO 7765-1
Coefficient of Friction >= 0.70>= 0.70film to film; ISO 8295
Film Tensile Strength at Break, MD 30.0 - 40.0 MPa4350 - 5800 psiISO 527-3
Film Tensile Strength at Break, TD 25.0 - 35.0 MPa3630 - 5080 psiISO 527-3
 
Thermal PropertiesMetricEnglishComments
Melting Point 133 - 136 °C271 - 277 °FISO 3146
Vicat Softening Point 115 °C
@Load 1.02 kg
239 °F
@Load 2.25 lb
A50; ISO 306
 
Optical PropertiesMetricEnglishComments
Haze <= 3.0 %<= 3.0 %ASTM D1003
Gloss >= 85 %>= 85 %20° of arc; ASTM D2457
Transmission, Visible 90 %90 %clear; thickness not quantified

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis Borclear™ RE936CF Polypropylene Random Copolymer
Borealis HB300TF Polypropylene
Borealis HJ320MO Polypropylene
Borealis RE216CF Polypropylene Random Copolymer
Dow R131-02A Polypropylene Random Copolymer Resin

PBOREA361 / 108621

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.