MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Eurotec® Tecomid® NA40 NL FA50 PA6.6, unfilled, flame retardant - halogen free, natural
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced, Flame Retardant

Material Notes:

Information provided by Eurotec®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.18 g/cc0.0426 lb/in³ISO 1183
Moisture Absorption 2.30 %
@Temperature 23.0 °C
2.30 %
@Temperature 73.4 °F
50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.013 cm/cm0.013 in/inEurotec
Linear Mold Shrinkage, Transverse 0.013 cm/cm0.013 in/inEurotec
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 80.0 MPa11600 psiISO 527
Tensile Modulus 3.75 GPa544 ksiISO 527
Izod Impact, Notched (ISO)  4.00 kJ/m²
@Temperature -30.0 °C
1.90 ft-lb/in²
@Temperature -22.0 °F
ISO 180/1A
 5.00 kJ/m²
@Temperature 23.0 °C
2.38 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1A
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohm1.00e+13 ohmIEC 60093
Comparative Tracking Index 600 V600 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 262 °C504 °F[10 K/min], ISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 255 °C491 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C176 °FISO 75
Vicat Softening Point 245 °C
@Load 5.10 kg
473 °F
@Load 11.2 lb
ISO 306
Flammability, UL94  V-0
@Thickness 0.750 mm
V-0
@Thickness 0.0295 in
 V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
Glow Wire Ignition Temperature 775 °C
@Thickness 2.00 mm
1430 °F
@Thickness 0.0787 in
IEC 60695
Glow Wire Flammability Index 960 °C
@Thickness 2.00 mm
1760 °F
@Thickness 0.0787 in
IEC 60695
 
Processing PropertiesMetricEnglishComments
Processing Temperature 260 - 280 °C500 - 536 °F
Feed Temperature 60.0 - 80.0 °C140 - 176 °FThroat
Mold Temperature 50.0 - 100 °C122 - 212 °F
Drying Temperature 80.0 °C176 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
Moisture Content <= 0.20 %<= 0.20 %ISO 960
Hold Pressure 50.0 - 100 MPa7250 - 14500 psi
 
Descriptive Properties
Back PressureLow
Injection SpeedMedium - Fast

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Eurotec® Tecolen® HP30 KG30 NL HS 0B PPCP, 30% glass fiber/glass bead reinforced, heat stabilized, natural
Eurotec® Tecomid® NA40 NL XA70 PA6.6, unfilled, flame retardant - halogen free (RoHS compliant), heat stabilized, natural
Covestro Bayblend® FR 3008 Polycarbonate + ABS, Flame Retardant Grade
Covestro Bayblend® FR 3008 HR Polycarbonate + ABS, Flame Retardant Grade
Covestro Bayblend® FR 3005 HF Polycarbonate + ABS, Flame Retardant Grade

PEUROS033 / 147023

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.