MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

PTS Trimid® N66-T100 Toughened Nylon 6/6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Impact Grade

Material Notes: Information provided by Polymer Technology and Services, LLC (PTS).

Key Words: Polyamide 66; PA66
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.08 g/cc0.0390 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 60.0 MPa8700 psiASTM D638
Elongation at Break 75 %75 %ASTM D638
Flexural Modulus 1.72 GPa249 ksiASTM D790
Izod Impact, Notched 2.40 J/cm
@Thickness 3.17 mm
4.50 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point 252 °C486 °FASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 71.0 °C160 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 254 °C490 °F
Middle Barrel Temperature 268 °C515 °F
Front Barrel Temperature 285 °C545 °F
Nozzle Temperature 266 - 282 °C510 - 540 °F
Melt Temperature 271 - 293 °C520 - 560 °F
Mold Temperature 26.7 - 93.3 °C80.0 - 200 °F
Drying Temperature 71.1 °C160 °F
Dry Time 4 hour4 hour
Injection Pressure 68.9 MPa10000 psi
Back Pressure 0.0689 - 0.689 MPa10.0 - 100 psi
Screw Speed 30 - 60 rpm30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyphthalamide (PPA)
Akro-Plastic Akromid® A3 1 S1 black (3616) PA66-I Conditioned
LATI Latamid 66 PA 66
GEHR Plastics PA 6.6-30GF Nylon 6.6, 30% Glass Fiber, Dry
Mitsubishi Chemical Advanced Materials Nylatron™ 101 / Ertalon™ 66 SA PA66 Extruded, Unfilled, Type 66 Natural and Black

PZ9PT57 / 21506

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.