MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

C.O.I.M. LARIPUR® LPR9060EF PTMG Polyether Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyether Grade

Material Notes: Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:
  • Excellent abrasion resistance
  • Great flexibility with constancy at temperature variations
  • Good compression resistance
  • Good water and light resistance
  • Good resistance to oils, fats and to many types of solvents

Series 60 and E 2103 PTMG Ether: These products are based on PTMG polyether. In comparison to the LARIPUR® ester series, they show a higher resistance to hydrolysis and microbiological attacks, have higher cold flexibility but have lower thermal and oxidizing resistance.
Information provided by P.A.T. Products, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.14 g/cc1.14 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8686ASTM D2240
Tensile Strength, Yield 43.3 MPa6280 psiASTM D412
Elongation at Break 580 %580 %ASTM D412
50% Modulus 5.00 MPa
@Strain 50 %
5.00 MPa
@Strain 50 %
ASTM D412
100% Modulus 6.80 MPa
@Strain 100 %
986 psi
@Strain 100 %
ASTM D412
300% Modulus 15.5 MPa
@Strain 300 %
2250 psi
@Strain 300 %
ASTM D412
Tear Strength 70.0 kN/m399 pliASTM D624
Abrasion 4040mm3, Abrasion Loss; DIN 53516
Compression Set 42 %
@Temperature 70.0 °C
42 %
@Temperature 158 °F
Method B, 22 hours; ASTM D395
 24 %
@Temperature 23.0 °C,
Time 252000 sec
24 %
@Temperature 73.4 °F,
Time 70.0 hour
ASTM D395
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 100 °C212 °FASTM D1525
Flammability, UL94 V-0V-0Vertical Burning
 
Descriptive Properties
FeaturesFlame Retardant, Transparent, Halogen Free

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
C.O.I.M. LARIPUR® LPR9060 PTMG Polyether Polyurethane
C.O.I.M. LARIPUR® LPR70D60 PTMG Polyether Polyurethane
C.O.I.M. LARIPUR® LPR9060EM PTMG Polyether Polyurethane
C.O.I.M. LARIPUR® LPR2103-90AE PTMG Polyether Polyurethane
C.O.I.M. LARIPUR® LPR5260 PTMG Polyether Polyurethane

PCOIM027 / 28630

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.