MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik Pleximid® 8817 PMMI Molding Compound
Categories: Polymer; Thermoplastic; Acrylic (PMMA)

Material Notes: Description: PLEXIMID® is a polymethyl methacrylimide (PMMI) product. This molding compound is characterized by its very high heat deflection temperature under load and rigidity. PLEXIMID® molding compounds are particularly suited for injection-molded parts for applications exposed to extreme thermal stress.

Information provided by degussa.

Evonik Industries is the successor company to Degussa.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.21 g/cc0.0437 lb/in³ISO 1183
Melt Flow 1.21 g/10 min
@Load 10.0 kg,
Temperature 260 °C
1.21 g/10 min
@Load 22.0 lb,
Temperature 500 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 90.0 MPa13100 psi5 mm/min; ISO 527
Elongation at Break 5.5 %5.5 %5 mm/min; ISO 527
Tensile Modulus 4.50 GPa653 ksi1 mm/min; ISO 527
Charpy Impact Unnotched 2.00 J/cm²
@Temperature 23.0 °C
9.52 ft-lb/in²
@Temperature 73.4 °F
ISO 179
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 166 °C331 °FISO 75
Vicat Softening Point 170 °C338 °FB50; ISO 306
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
IEC 707
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.541.54ISO 489
Transmission, Visible 90 %90 %Transmission Factor; DIN 5036

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik Pleximid® 8813 PMMI Molding Compound
Covestro Apec® 1803 Polycarbonate
Evonik Pleximid® 8805 PMMI Molding Compound
Röhm Acrylite® 249 Acrylic Sheet, Aerospace Grade
Skybond® 9100 Aromatic Polyimide Resin for RTM Molding

PHUK063 / 47197

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.