MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Nylene® PA6/6 Impact Modified 4114 HS Nylon 6/6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Impact Grade

Material Notes: High Impact Grade; Property data for dry as molded samples.

ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.

Key Words: Polyamide 66; Nylon 66
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.07 g/cc0.0387 lb/in³
Linear Mold Shrinkage 0.0070 cm/cm0.0070 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 51.0 MPa7400 psiASTM D638
Elongation at Break 55 %55 %ASTM D638
Flexural Modulus 1.71 GPa248 ksiASTM D790
Izod Impact, Notched 9.99 J/cm18.7 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point 254 °C489 °FASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 68.0 °C154 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Nylene® PA6/6 Glass Filled 5133 HS Nylon 6/6
Covestro Makroblend® UT-408 Polycarbonate + Polyester Blend
Covestro Makroblend® UT-1018 Polycarbonate + Polyester Blend
Celanese Celcon® M90™ POM, Unfilled
INEOS Styrolution Terluran® GP-35 ABS

PNY6C6 / 55518

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.