MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Overview of materials for High Density Polyethylene (HDPE), Impact Grade
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Impact Grade

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Impact Grade". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 0.945 - 0.962 g/cc0.0341 - 0.0348 lb/in³Average value: 0.951 g/cc Grade Count:16
Viscosity  39000 - 480000 cP
@Temperature 190 - 190 °C
39000 - 480000 cP
@Temperature 374 - 374 °F
Average value: 164000 cP Grade Count:7
 39000 - 480000 cP
@Shear Rate 300 - 5000 1/s
39000 - 480000 cP
@Shear Rate 300 - 5000 1/s
Average value: 164000 cP Grade Count:7
Environmental Stress Crack Resistance 1.00 - 500 hour1.00 - 500 hourAverage value: 202 hour Grade Count:4
Melt Flow 0.300 - 42.0 g/10 min0.300 - 42.0 g/10 minAverage value: 14.5 g/10 min Grade Count:16
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 59.0 - 64.059.0 - 64.0Average value: 61.0 Grade Count:4
Tensile Strength, Ultimate 10.0 - 27.0 MPa1450 - 3920 psiAverage value: 15.1 MPa Grade Count:9
Tensile Strength, Yield 17.2 - 25.0 MPa2490 - 3630 psiAverage value: 21.6 MPa Grade Count:16
Elongation at Break 50.0 - 1000 %50.0 - 1000 %Average value: 448 % Grade Count:16
Modulus of Elasticity 0.510 - 1.10 GPa74.0 - 160 ksiAverage value: 0.702 GPa Grade Count:10
Flexural Modulus 0.772 - 1.17 GPa112 - 170 ksiAverage value: 0.907 GPa Grade Count:13
Izod Impact, Notched 0.534 - 3.74 J/cm1.00 - 7.00 ft-lb/inAverage value: 1.60 J/cm Grade Count:3
Izod Impact, Notched (ISO) 27.0 - 176 kJ/m²12.8 - 83.7 ft-lb/in²Average value: 75.7 kJ/m² Grade Count:8
Falling Dart Impact 32.5397 - 176.257 J
@Temperature -40.0 - -40.0 °C
24.0000 - 130.000 ft-lb
@Temperature -40.0 - -40.0 °F
Average value: 104 J Grade Count:2
 
Thermal PropertiesMetricEnglishComments
Melting Point 128 - 133 °C262 - 271 °FAverage value: 131 °C Grade Count:3
Deflection Temperature at 0.46 MPa (66 psi) 66.0 - 73.0 °C151 - 163 °FAverage value: 70.5 °C Grade Count:4
Vicat Softening Point 75.0 - 129 °C167 - 264 °FAverage value: 115 °C Grade Count:12
Brittleness Temperature -118 - -75.0 °C-180 - -103 °FAverage value: -94.3 °C Grade Count:4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for High Density Polyethylene (HDPE), Injection Molded
Overview of materials for High Density Polyethylene (HDPE), Extruded
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight
Overview of materials for High Density Polyethylene (HDPE), Rotational Molding Grade
Overview of materials for High Density Polyethylene (HDPE), Crosslinkable

O4002 / 78277

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.