MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

LyondellBasell Purell RP320M Polypropylene
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Purell RP320M is a controlled rheology medium modified polypropylene random copolymer. It does not contain slip or anti-blocking additives. Purell RP320M is typically used for manufacturing of un-oriented cast films. Customer report lamination, textile and packaging of foodstuffs as typical applications. Purell RP320M exhibits good processability, and that films produced with Purell RP320M exhibits high clarity and gloss, softness and good heat weldability. Applications: Caps & Closures (Healthcare), Healthcare Applications, Medical Film.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ISO 1183-1
Melt Flow 8.5 g/10 min
@Load 2.16 kg,
Temperature 230 °C
8.5 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 25.0 MPa3630 psiISO 527-1,-2
Elongation at Break >= 50 %>= 50 %ISO 527-1,-2
Elongation at Yield 13 %13 %ISO 527-1,-2
Tensile Modulus 0.850 GPa123 ksiISO 527-1,-2
Charpy Impact, Notched  0.200 J/cm²
@Temperature 0.000 °C
0.952 ft-lb/in²
@Temperature 32.0 °F
ISO 179-1/1eA
 0.700 J/cm²
@Temperature 23.0 °C
3.33 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 68.0 °C154 °Funannealed; ISO 75B-1,-2
Vicat Softening Point 135 °C275 °FA50; ISO 306
 
Descriptive Properties
Processing MethodCast Film, Injection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Braskem RP250 Polypropylene Random Copolymer
Bamberger Polymers Bapolene® 5063C Polypropylene, Injection Grade
Dow 6D20 Polypropylene Random Copolymer Resin
Flint Hills P9R6K-054A Random Copolymer Polypropylene
I. Stern 2335C Prime Clarified Random Copolymer Polypropylene

PEQT8643 / 220277

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.