MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Röhm Acrylite® AR Acrylic Sheet, Abrasion Resistant  (discontinued **)
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Optical Sheet

Material Notes: Data provided by CYRO Industries

Continuously manufactured sheet with an abrasion and chemical resistant coating. Available with one or both sides coated.

Information Provided by Evonik CYRO. The former Evonik Methacrylates business has been sold to Röhm (Roehm) GmbH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.19 g/cc0.0430 lb/in³typical of Acrylite® sheet
 
Mechanical PropertiesMetricEnglishComments
Elongation at Break 4.5 %4.5 %ASTM D638
Tensile Modulus 2.80 GPa406 ksiASTM D638
Flexural Yield Strength 117 MPa17000 psiASTM D790
Flexural Modulus 3.30 GPa479 ksiASTM D790
Izod Impact, Notched 0.216 J/cm0.405 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear 68.0 µm/m-°C
@Temperature 20.0 °C
37.8 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Specific Heat Capacity 1.47 J/g-°C0.351 BTU/lb-°Ftypical of Acrylite® sheet
Thermal Conductivity 0.190 W/m-K1.32 BTU-in/hr-ft²-°F
Deflection Temperature at 1.8 MPa (264 psi) 91.0 °C196 °FASTM D648
Vicat Softening Point 105 °C221 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 92 %92 %ASTM D1003

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Röhm Acrylite® 8N Acrylic Polymer
INEOS Styrolution Zylar® 960 MBS
Plaskolite Optix® Acrylic Sheet
Röhm ACRYLITE® GAR Abrasion Resistant Cell Cast Acrylic Sheet
Röhm Acrylite® GP Acrylic Sheet, Cast

PCYR32 / 29171

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.